[vendor]
|
||
repo_id = orcaslicer-fff
|
||
name = OrcaFilamentLibrary
|
||
config_version = 02.03.02.60
|
||
description = Orca Filament Library
|
||
force_update = 0
|
||
|
||
[filament:fdm_filament_common]
|
||
from = system
|
||
instantiation = false
|
||
activate_air_filtration = 0
|
||
chamber_temperatures = 0
|
||
close_fan_the_first_x_layers = 3
|
||
complete_print_exhaust_fan_speed = 70
|
||
cool_plate_temp = 60
|
||
cool_plate_temp_initial_layer = 60
|
||
during_print_exhaust_fan_speed = 70
|
||
eng_plate_temp = 60
|
||
eng_plate_temp_initial_layer = 60
|
||
fan_cooling_layer_time = 60
|
||
fan_max_speed = 100
|
||
fan_min_speed = 35
|
||
filament_cost = 0
|
||
filament_density = 0
|
||
filament_deretraction_speed = nil
|
||
filament_diameter = 1.75
|
||
filament_flow_ratio = 1
|
||
filament_is_support = 0
|
||
filament_long_retractions_when_cut = nil
|
||
filament_max_volumetric_speed = 0
|
||
filament_minimal_purge_on_wipe_tower = 15
|
||
filament_retract_before_wipe = nil
|
||
filament_retract_restart_extra = nil
|
||
filament_retract_when_changing_layer = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
filament_retraction_length = nil
|
||
filament_retraction_minimum_travel = nil
|
||
filament_retraction_speed = nil
|
||
filament_settings_id =
|
||
filament_soluble = 0
|
||
filament_type = PLA
|
||
filament_vendor = Generic
|
||
filament_wipe = nil
|
||
filament_wipe_distance = nil
|
||
filament_z_hop = nil
|
||
filament_z_hop_types = nil
|
||
full_fan_speed_layer = 0
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_height = 10%
|
||
filament_scarf_gap = 0%
|
||
filament_scarf_length = 10
|
||
filament_shrink = 100%
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
nozzle_temperature = 200
|
||
nozzle_temperature_initial_layer = 200
|
||
overhang_fan_speed = 100
|
||
overhang_fan_threshold = 95%
|
||
reduce_fan_stop_start_freq = 0
|
||
required_nozzle_HRC = 3
|
||
supertack_plate_temp = 45
|
||
supertack_plate_temp_initial_layer = 45
|
||
slow_down_for_layer_cooling = 1
|
||
slow_down_layer_time = 8
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 100
|
||
textured_plate_temp = 60
|
||
textured_plate_temp_initial_layer = 60
|
||
filament_start_gcode = ; Filament gcode
|
||
|
||
filament_end_gcode = ; filament end gcode
|
||
|
||
compatible_printers =
|
||
|
||
[filament:FusRock ABS-GF @base]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFR00
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials(https://wiki.fusrock.com).
|
||
filament_extruder_variant = Direct Drive Standard
|
||
filament_adhesiveness_category = 200
|
||
filament_type = ABS-GF
|
||
filament_vendor = FusRock
|
||
filament_flow_ratio = 0.92
|
||
filament_density = 1.08
|
||
filament_cost = 13
|
||
nozzle_temperature_range_low = 240
|
||
nozzle_temperature_range_high = 280
|
||
cool_plate_temp_initial_layer = 0
|
||
cool_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
supertack_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 105
|
||
eng_plate_temp = 105
|
||
hot_plate_temp_initial_layer = 105
|
||
hot_plate_temp = 105
|
||
textured_plate_temp_initial_layer = 105
|
||
textured_plate_temp = 105
|
||
nozzle_temperature_initial_layer = 260
|
||
nozzle_temperature = 270
|
||
filament_max_volumetric_speed = 18
|
||
close_fan_the_first_x_layers = 3
|
||
fan_min_speed = 10
|
||
fan_cooling_layer_time = 12
|
||
fan_max_speed = 30
|
||
slow_down_layer_time = 4
|
||
reduce_fan_stop_start_freq = 0
|
||
slow_down_for_layer_cooling = 1
|
||
slow_down_min_speed = 20
|
||
enable_overhang_bridge_fan = 1
|
||
overhang_fan_threshold = 10%
|
||
overhang_threshold_participating_cooling = 100%
|
||
overhang_fan_speed = 30
|
||
pre_start_fan_time = 0
|
||
additional_cooling_fan_speed = 0
|
||
activate_air_filtration = 1
|
||
during_print_exhaust_fan_speed = 30
|
||
complete_print_exhaust_fan_speed = 10
|
||
filament_retraction_length = 0.8
|
||
filament_z_hop = 0.4
|
||
filament_z_hop_types = Spiral Lift
|
||
filament_retraction_speed = 30
|
||
filament_deretraction_speed = 0
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_when_changing_layer = 0
|
||
filament_wipe = 0
|
||
filament_wipe_distance = 2
|
||
filament_retract_before_wipe = 100%
|
||
filament_end_gcode = ; filament end gcode
|
||
|
||
|
||
filament_notes = //EN
|
||
1.Be sure to read it carefully before using (https://wiki.fusrock.com).
|
||
2.When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials(https://wiki.fusrock.com).\n3.Thank you for choosing us FusRock.
|
||
*This setting may not be able to adapt to all models. In some cases, you need to modify and adjust the parameters by yourself to improve the printing effect.
|
||
*FusRock 3D printing filaments are intended for general-purpose printing and have been tested under standard conditions. However, the performance and safety of printed objects are affected by multiple factors, including printing parameters, model design, usage environment, and the specific application.
|
||
*By using FusRock materials, the user acknowledges and agrees to independently evaluate whether the printed parts are suitable for their intended use, and assumes all associated risks.
|
||
*FusRock shall not be held liable for any damage, injury, or loss that may result from the use of printed products made with our materials, including but not limited to structural failure, functional defects, or safety hazards under actual usage conditions.Before applying printed parts in any critical, functional, or commercial context, thorough testing must be conducted. Except for the certifications explicitly stated for specific FusRock materials, our products are not certified for medical, aerospace, or life-support applications.
|
||
//CN
|
||
1.使用前请务必仔细阅读(https://wiki.fusrock.com)。
|
||
2.打印该耗材时,可能会出现喷嘴堵塞、拉丝、翘边以及层间附着力不足等问题。为了获得更好的打印效果,请参考此维基页面:高温 / 工程材料打印技巧(https://wiki.fusrock.com)。
|
||
3.感谢您选择FusRock。
|
||
*此设置不一定能够适配所有模型,存在部分情况下需要您自行修改调整参数来提升打印效果。
|
||
*FusRock 3D打印耗材适用于通用打印用途,已在标准条件下进行测试。然而,打印成品的性能与安全性受多种因素影响,包括打印参数、模型设计、使用环境及实际用途。
|
||
*使用FusRock材料即表示用户已知悉并同意,自行评估打印件是否适用于其具体应用,并承担由此产生的全部风险。
|
||
*FusRock对使用本公司耗材打印的产品在实际应用中可能导致的任何损害、伤害或损失不承担任何责任,包括但不限于结构失效、功能异常或使用环境中的安全隐患。在将打印件应用于关键、功能性或商业性场景前,请务必进行充分测试。除FusRock已标明材料所获得的各项认证资质外,FusRock产品未取得医疗、航天或生命支持系统认证资质。
|
||
impact_strength_z = 5.3
|
||
|
||
[filament:fdm_filament_abs]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
instantiation = false
|
||
activate_air_filtration = 0
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 100
|
||
eng_plate_temp_initial_layer = 105
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 80
|
||
fan_min_speed = 10
|
||
filament_cost = 20
|
||
filament_density = 1.04
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = ABS
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 105
|
||
nozzle_temperature = 260
|
||
nozzle_temperature_initial_layer = 260
|
||
nozzle_temperature_range_high = 280
|
||
nozzle_temperature_range_low = 240
|
||
overhang_fan_speed = 80
|
||
overhang_fan_threshold = 25%
|
||
reduce_fan_stop_start_freq = 1
|
||
slow_down_layer_time = 3
|
||
slow_down_min_speed = 10
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 105
|
||
filament_flow_ratio = 0.926
|
||
temperature_vitrification = 110
|
||
|
||
[filament:fdm_filament_asa]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
instantiation = false
|
||
activate_air_filtration = 0
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 100
|
||
eng_plate_temp_initial_layer = 105
|
||
fan_cooling_layer_time = 35
|
||
fan_max_speed = 80
|
||
fan_min_speed = 10
|
||
filament_cost = 20
|
||
filament_density = 1.04
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = ASA
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 105
|
||
nozzle_temperature = 260
|
||
nozzle_temperature_initial_layer = 260
|
||
nozzle_temperature_range_high = 280
|
||
nozzle_temperature_range_low = 240
|
||
overhang_fan_speed = 80
|
||
overhang_fan_threshold = 25%
|
||
reduce_fan_stop_start_freq = 1
|
||
slow_down_layer_time = 3
|
||
slow_down_min_speed = 10
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 105
|
||
filament_flow_ratio = 0.926
|
||
temperature_vitrification = 110
|
||
|
||
[filament:fdm_filament_bvoh]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFS97
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 70
|
||
close_fan_the_first_x_layers = 1
|
||
cool_plate_temp = 40
|
||
cool_plate_temp_initial_layer = 40
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 69.99
|
||
filament_density = 1.13
|
||
filament_is_support = 1
|
||
filament_max_volumetric_speed = 8
|
||
filament_type = BVOH
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
overhang_fan_threshold = 50%
|
||
reduce_fan_stop_start_freq = 1
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 45
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
|
||
[filament:fdm_filament_cope]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFLC99
|
||
instantiation = false
|
||
filament_type = CoPE
|
||
additional_cooling_fan_speed = 70
|
||
close_fan_the_first_x_layers = 1
|
||
cool_plate_temp = 35
|
||
cool_plate_temp_initial_layer = 35
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 20
|
||
filament_density = 1.29
|
||
filament_max_volumetric_speed = 16
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_gap = 15%
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_low = 190
|
||
nozzle_temperature_range_high = 240
|
||
overhang_fan_threshold = 50%
|
||
reduce_fan_stop_start_freq = 1
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 45
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
filament_flow_ratio = 0.98
|
||
|
||
[filament:fdm_filament_eva]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFR99
|
||
instantiation = false
|
||
filament_type = EVA
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
|
||
[filament:fdm_filament_hips]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFS98
|
||
instantiation = false
|
||
cool_plate_temp = 0
|
||
eng_plate_temp = 90
|
||
hot_plate_temp = 90
|
||
textured_plate_temp = 90
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp_initial_layer = 90
|
||
hot_plate_temp_initial_layer = 90
|
||
textured_plate_temp_initial_layer = 90
|
||
fan_cooling_layer_time = 10
|
||
filament_max_volumetric_speed = 8
|
||
filament_type = HIPS
|
||
filament_density = 1.06
|
||
filament_cost = 22.99
|
||
nozzle_temperature_initial_layer = 240
|
||
fan_max_speed = 60
|
||
fan_min_speed = 0
|
||
overhang_fan_threshold = 25%
|
||
overhang_fan_speed = 80
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_range_low = 220
|
||
nozzle_temperature_range_high = 270
|
||
slow_down_min_speed = 10
|
||
slow_down_layer_time = 6
|
||
additional_cooling_fan_speed = 0
|
||
|
||
[filament:fdm_filament_pa]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFN99
|
||
instantiation = false
|
||
activate_air_filtration = 0
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 100
|
||
eng_plate_temp_initial_layer = 100
|
||
fan_cooling_layer_time = 4
|
||
fan_max_speed = 60
|
||
fan_min_speed = 0
|
||
filament_cost = 20
|
||
filament_density = 1.04
|
||
filament_max_volumetric_speed = 8
|
||
filament_type = PA
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 100
|
||
nozzle_temperature = 280
|
||
nozzle_temperature_initial_layer = 280
|
||
nozzle_temperature_range_high = 300
|
||
nozzle_temperature_range_low = 260
|
||
overhang_fan_speed = 30
|
||
required_nozzle_HRC = 40
|
||
slow_down_layer_time = 2
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 108
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 100
|
||
|
||
[filament:fdm_filament_paht]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
instantiation = false
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PAHT
|
||
filament_density = 1.24
|
||
filament_cost = 0
|
||
cool_plate_temp = 35
|
||
eng_plate_temp = 0
|
||
textured_plate_temp = 60
|
||
cool_plate_temp_initial_layer = 35
|
||
eng_plate_temp_initial_layer = 0
|
||
textured_plate_temp_initial_layer = 60
|
||
nozzle_temperature_initial_layer = 220
|
||
reduce_fan_stop_start_freq = 1
|
||
overhang_fan_threshold = 50%
|
||
close_fan_the_first_x_layers = 1
|
||
nozzle_temperature = 220
|
||
temperature_vitrification = 45
|
||
nozzle_temperature_range_low = 190
|
||
nozzle_temperature_range_high = 240
|
||
slow_down_min_speed = 20
|
||
additional_cooling_fan_speed = 0
|
||
fan_cooling_layer_time = 80
|
||
fan_min_speed = 50
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
slow_down_layer_time = 8
|
||
filament_start_gcode = ; Filament start gcode
|
||
|
||
filament_end_gcode = ; filament end gcode
|
||
|
||
filament_vendor = Generic
|
||
|
||
[filament:fdm_filament_pc]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFC99
|
||
instantiation = false
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 110
|
||
eng_plate_temp_initial_layer = 110
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 60
|
||
fan_min_speed = 10
|
||
filament_cost = 20
|
||
filament_density = 1.04
|
||
filament_type = PC
|
||
hot_plate_temp = 110
|
||
hot_plate_temp_initial_layer = 110
|
||
nozzle_temperature = 280
|
||
nozzle_temperature_initial_layer = 270
|
||
nozzle_temperature_range_high = 290
|
||
nozzle_temperature_range_low = 260
|
||
overhang_fan_speed = 60
|
||
overhang_fan_threshold = 25%
|
||
reduce_fan_stop_start_freq = 1
|
||
slow_down_layer_time = 2
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 120
|
||
textured_plate_temp = 110
|
||
textured_plate_temp_initial_layer = 110
|
||
filament_max_volumetric_speed = 12
|
||
filament_flow_ratio = 0.94
|
||
|
||
[filament:fdm_filament_pctg]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFG97
|
||
instantiation = false
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 20
|
||
fan_min_speed = 20
|
||
filament_cost = 30
|
||
filament_density = 1.27
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PCTG
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 80
|
||
nozzle_temperature = 255
|
||
nozzle_temperature_initial_layer = 255
|
||
nozzle_temperature_range_high = 260
|
||
nozzle_temperature_range_low = 220
|
||
reduce_fan_stop_start_freq = 1
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
temperature_vitrification = 70
|
||
textured_plate_temp = 80
|
||
textured_plate_temp_initial_layer = 80
|
||
|
||
[filament:fdm_filament_pe]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFP99
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 70
|
||
close_fan_the_first_x_layers = 1
|
||
cool_plate_temp = 35
|
||
cool_plate_temp_initial_layer = 35
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 20
|
||
filament_density = 1.24
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PE
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
overhang_fan_threshold = 50%
|
||
reduce_fan_stop_start_freq = 1
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 45
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
|
||
[filament:fdm_filament_pet]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFG99
|
||
instantiation = false
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 20
|
||
fan_min_speed = 20
|
||
filament_cost = 30
|
||
filament_density = 1.27
|
||
filament_max_volumetric_speed = 10
|
||
filament_type = PETG
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 80
|
||
nozzle_temperature = 255
|
||
nozzle_temperature_initial_layer = 255
|
||
nozzle_temperature_range_high = 260
|
||
nozzle_temperature_range_low = 220
|
||
reduce_fan_stop_start_freq = 1
|
||
supertack_plate_temp = 70
|
||
supertack_plate_temp_initial_layer = 70
|
||
temperature_vitrification = 70
|
||
textured_plate_temp = 80
|
||
textured_plate_temp_initial_layer = 80
|
||
|
||
[filament:fdm_filament_pha]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFR98
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 70
|
||
close_fan_the_first_x_layers = 1
|
||
cool_plate_temp = 35
|
||
cool_plate_temp_initial_layer = 35
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 27.99
|
||
filament_density = 1.24
|
||
filament_max_volumetric_speed = 6
|
||
filament_type = PHA
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
overhang_fan_threshold = 50%
|
||
reduce_fan_stop_start_freq = 1
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 120
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
|
||
[filament:fdm_filament_pla]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFL99
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 70
|
||
close_fan_the_first_x_layers = 1
|
||
cool_plate_temp = 35
|
||
cool_plate_temp_initial_layer = 35
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 20
|
||
filament_density = 1.24
|
||
filament_max_volumetric_speed = 12
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_gap = 15%
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_low = 190
|
||
nozzle_temperature_range_high = 240
|
||
overhang_fan_threshold = 50%
|
||
reduce_fan_stop_start_freq = 1
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 45
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
filament_flow_ratio = 0.98
|
||
|
||
[filament:fdm_filament_pp]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFP97
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 70
|
||
close_fan_the_first_x_layers = 1
|
||
cool_plate_temp = 35
|
||
cool_plate_temp_initial_layer = 35
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 34.99
|
||
filament_density = 0.93
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PP
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
nozzle_temperature = 235
|
||
nozzle_temperature_initial_layer = 235
|
||
nozzle_temperature_range_high = 250
|
||
nozzle_temperature_range_low = 220
|
||
overhang_fan_threshold = 50%
|
||
reduce_fan_stop_start_freq = 1
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 110
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
|
||
[filament:fdm_filament_ppa]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OGFN97
|
||
instantiation = false
|
||
activate_air_filtration = 0
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 100
|
||
eng_plate_temp_initial_layer = 100
|
||
fan_cooling_layer_time = 5
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 20
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.96
|
||
filament_max_volumetric_speed = 8
|
||
filament_type = PPA-CF
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 100
|
||
nozzle_temperature = 290
|
||
nozzle_temperature_initial_layer = 290
|
||
nozzle_temperature_range_high = 320
|
||
nozzle_temperature_range_low = 280
|
||
overhang_fan_speed = 40
|
||
overhang_fan_threshold = 0%
|
||
required_nozzle_HRC = 40
|
||
slow_down_layer_time = 2
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 210
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 100
|
||
|
||
[filament:fdm_filament_pps]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
instantiation = false
|
||
chamber_temperatures = 60
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 110
|
||
eng_plate_temp_initial_layer = 110
|
||
fan_cooling_layer_time = 5
|
||
fan_max_speed = 50
|
||
fan_min_speed = 0
|
||
filament_density = 1.36
|
||
filament_flow_ratio = 0.96
|
||
filament_max_volumetric_speed = 4
|
||
filament_type = PPS
|
||
hot_plate_temp = 110
|
||
hot_plate_temp_initial_layer = 110
|
||
nozzle_temperature = 320
|
||
nozzle_temperature_initial_layer = 320
|
||
nozzle_temperature_range_high = 340
|
||
nozzle_temperature_range_low = 300
|
||
overhang_fan_speed = 30
|
||
overhang_fan_threshold = 0%
|
||
slow_down_layer_time = 2
|
||
temperature_vitrification = 125
|
||
textured_plate_temp = 110
|
||
textured_plate_temp_initial_layer = 110
|
||
|
||
[filament:fdm_filament_pva]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 70
|
||
close_fan_the_first_x_layers = 1
|
||
cool_plate_temp = 45
|
||
cool_plate_temp_initial_layer = 45
|
||
eng_plate_temp = 0
|
||
eng_plate_temp_initial_layer = 0
|
||
fan_cooling_layer_time = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 20
|
||
filament_density = 1.24
|
||
filament_is_support = 1
|
||
filament_max_volumetric_speed = 12
|
||
filament_soluble = 1
|
||
filament_type = PVA
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
overhang_fan_threshold = 50%
|
||
reduce_fan_stop_start_freq = 1
|
||
supertack_plate_temp = 35
|
||
supertack_plate_temp_initial_layer = 35
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 45
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
filament_flow_ratio = 0.95
|
||
|
||
[filament:fdm_filament_sbs]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
filament_id = OFLSBS99
|
||
instantiation = false
|
||
fan_cooling_layer_time = 100
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = SBS
|
||
filament_density = 1.02
|
||
filament_cost = 15
|
||
cool_plate_temp = 70
|
||
eng_plate_temp = 70
|
||
hot_plate_temp = 70
|
||
textured_plate_temp = 70
|
||
cool_plate_temp_initial_layer = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
nozzle_temperature_initial_layer = 235
|
||
reduce_fan_stop_start_freq = 0
|
||
fan_min_speed = 0
|
||
overhang_fan_threshold = 50%
|
||
close_fan_the_first_x_layers = 3
|
||
nozzle_temperature = 235
|
||
temperature_vitrification = 70
|
||
nozzle_temperature_range_low = 215
|
||
nozzle_temperature_range_high = 250
|
||
slow_down_min_speed = 10
|
||
slow_down_layer_time = 4
|
||
additional_cooling_fan_speed = 40
|
||
|
||
[filament:fdm_filament_tpu]
|
||
inherits = fdm_filament_common
|
||
from = system
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 70
|
||
close_fan_the_first_x_layers = 1
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
cool_plate_temp = 30
|
||
cool_plate_temp_initial_layer = 30
|
||
eng_plate_temp = 30
|
||
eng_plate_temp_initial_layer = 30
|
||
fan_cooling_layer_time = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 20
|
||
filament_density = 1.24
|
||
filament_max_volumetric_speed = 3.2
|
||
filament_retraction_length = 0.4
|
||
filament_type = TPU
|
||
hot_plate_temp = 35
|
||
hot_plate_temp_initial_layer = 35
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 240
|
||
nozzle_temperature_range_high = 250
|
||
nozzle_temperature_range_low = 200
|
||
reduce_fan_stop_start_freq = 1
|
||
temperature_vitrification = 30
|
||
textured_plate_temp = 35
|
||
textured_plate_temp_initial_layer = 35
|
||
|
||
[filament:FusRock ABS-GF @System]
|
||
inherits = FusRock ABS-GF @base
|
||
from = system
|
||
setting_id = OGFSB50_00
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu ABS @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = OGFB00
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 24.99
|
||
filament_flow_ratio = 0.95
|
||
filament_vendor = Bambu Lab
|
||
|
||
[filament:Bambu ABS-GF @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = OGFB50
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
fan_cooling_layer_time = 12
|
||
fan_max_speed = 30
|
||
filament_cost = 29.99
|
||
filament_density = 1.08
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = ABS-GF
|
||
filament_vendor = Bambu Lab
|
||
overhang_fan_speed = 30
|
||
overhang_fan_threshold = 10%
|
||
slow_down_layer_time = 4
|
||
|
||
[filament:Bambu Support for ABS @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = OGFS06
|
||
instantiation = false
|
||
description = This is a non-water-soluble support filament, and usually it is only for the support structure and not for the model body. To get better printing quality, please refer to this wiki: Printing Tips for Support Filament and Support Function.
|
||
fan_max_speed = 30
|
||
filament_cost = 29.98
|
||
filament_flow_ratio = 0.95
|
||
filament_is_support = 1
|
||
filament_max_volumetric_speed = 6
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature_range_high = 270
|
||
slow_down_layer_time = 12
|
||
filament_scarf_seam_type = none
|
||
temperature_vitrification = 90
|
||
|
||
[filament:COEX ABS @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = CXABSB01
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 30.00
|
||
filament_density = 1.04
|
||
filament_type = ABS
|
||
nozzle_temperature = 255
|
||
nozzle_temperature_initial_layer = 255
|
||
bed_temperature = 100
|
||
bed_temperature_initial_layer = 100
|
||
temperature_vitrification = 100
|
||
chamber_temperature = 0
|
||
filament_max_volumetric_speed = 16
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 2.5
|
||
filament_retraction_speed = 40
|
||
filament_deretraction_speed = 40
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 0
|
||
fan_max_speed = 30
|
||
disable_fan_first_layers = 3
|
||
full_fan_speed_layer = 0
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
enable_pressure_advance = 1
|
||
pressure_advance = 0.04
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:COEX ABS PRIME @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = CXABPB09
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 39.00
|
||
filament_density = 1.04
|
||
filament_type = ABS
|
||
nozzle_temperature = 255
|
||
nozzle_temperature_initial_layer = 255
|
||
bed_temperature = 100
|
||
bed_temperature_initial_layer = 100
|
||
temperature_vitrification = 100
|
||
chamber_temperature = 0
|
||
filament_max_volumetric_speed = 16
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 2.5
|
||
filament_retraction_speed = 40
|
||
filament_deretraction_speed = 40
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 0
|
||
fan_max_speed = 30
|
||
disable_fan_first_layers = 3
|
||
full_fan_speed_layer = 0
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
enable_pressure_advance = 1
|
||
pressure_advance = 0.04
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:Elegoo ABS @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = EABSB00
|
||
instantiation = false
|
||
filament_vendor = Elegoo
|
||
filament_density = 1.1
|
||
filament_max_volumetric_speed = 12
|
||
nozzle_temperature = 270
|
||
fan_cooling_layer_time = 35
|
||
|
||
[filament:Eolas Prints ABS @System]
|
||
filament_id = GFSEP017
|
||
setting_id = GFSEP017_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_abs
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = ABS
|
||
nozzle_temperature = 255
|
||
nozzle_temperature_initial_layer = 260
|
||
nozzle_temperature_range_low = 240
|
||
nozzle_temperature_range_high = 270
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 105
|
||
chamber_temperature = 40
|
||
filament_density = 1.04
|
||
filament_cost = 19.50
|
||
filament_spool_weight = 900
|
||
filament_max_volumetric_speed = 18
|
||
|
||
[filament:FDplast ABS @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = FDPLAST01
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 11
|
||
default_filament_colour =
|
||
filament_vendor = FDplast
|
||
filament_flow_ratio = 0.95
|
||
nozzle_temperature_range_high = 260
|
||
nozzle_temperature_range_low = 245
|
||
|
||
[filament:Generic ABS @System]
|
||
renamed_from = My Generic ABS
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFB99
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:NIT ABS @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = NIT01
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 10
|
||
default_filament_colour =
|
||
filament_flow_ratio = 0.95
|
||
filament_vendor = NIT
|
||
|
||
[filament:Overture ABS Basic @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = OVTABS08
|
||
instantiation = false
|
||
description = Overture ABS settings from https://overture3d.com/.
|
||
activate_air_filtration = 1
|
||
additional_cooling_fan_speed = 0
|
||
chamber_temperatures = 0
|
||
close_fan_the_first_x_layers = 3
|
||
compatible_printers =
|
||
complete_print_exhaust_fan_speed = 70
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
default_filament_colour =
|
||
during_print_exhaust_fan_speed = 70
|
||
enable_overhang_bridge_fan = 1
|
||
enable_pressure_advance = 0
|
||
eng_plate_temp = 90
|
||
eng_plate_temp_initial_layer = 90
|
||
fan_cooling_layer_time = 38
|
||
fan_max_speed = 50
|
||
fan_min_speed = 10
|
||
filament_cost = 0
|
||
filament_density = 1.15
|
||
filament_deretraction_speed = nil
|
||
filament_diameter = 1.75
|
||
filament_end_gcode = ; filament end gcode
|
||
M106 P3 S0
|
||
|
||
filament_flow_ratio = 0.95
|
||
filament_is_support = 0
|
||
filament_long_retractions_when_cut = nil
|
||
filament_max_volumetric_speed = 16
|
||
filament_minimal_purge_on_wipe_tower = 15
|
||
filament_notes =
|
||
filament_retract_before_wipe = nil
|
||
filament_retract_restart_extra = nil
|
||
filament_retract_when_changing_layer = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
filament_retraction_length = nil
|
||
filament_retraction_minimum_travel = nil
|
||
filament_retraction_speed = nil
|
||
filament_settings_id = OVERTURE ABS Basic
|
||
filament_soluble = 0
|
||
filament_start_gcode = ; Filament gcode
|
||
{if activate_air_filtration[current_extruder] && support_air_filtration}
|
||
M106 P3 S{during_print_exhaust_fan_speed_num[current_extruder]}
|
||
{endif}
|
||
filament_type = ABS
|
||
filament_vendor = Overture
|
||
filament_wipe = nil
|
||
filament_wipe_distance = nil
|
||
filament_z_hop = nil
|
||
filament_z_hop_types = nil
|
||
full_fan_speed_layer = 0
|
||
hot_plate_temp = 90
|
||
hot_plate_temp_initial_layer = 90
|
||
nozzle_temperature = 260
|
||
nozzle_temperature_initial_layer = 260
|
||
nozzle_temperature_range_high = 265
|
||
nozzle_temperature_range_low = 245
|
||
overhang_fan_speed = 100
|
||
overhang_fan_threshold = 95%
|
||
pressure_advance = 0.02
|
||
reduce_fan_stop_start_freq = 1
|
||
required_nozzle_HRC = 3
|
||
slow_down_for_layer_cooling = 1
|
||
slow_down_layer_time = 2
|
||
slow_down_min_speed = 20
|
||
temperature_vitrification = 103
|
||
textured_plate_temp = 90
|
||
textured_plate_temp_initial_layer = 90
|
||
|
||
[filament:PolyLite ABS @base]
|
||
inherits = fdm_filament_abs
|
||
from = system
|
||
filament_id = OGFB60
|
||
instantiation = false
|
||
filament_cost = 26.9
|
||
filament_density = 1.03
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Polymaker
|
||
|
||
[filament:Bambu ASA @base]
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
filament_id = OGFB01
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
eng_plate_temp = 100
|
||
eng_plate_temp_initial_layer = 100
|
||
fan_max_speed = 35
|
||
filament_cost = 31.99
|
||
filament_density = 1.05
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Bambu Lab
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 100
|
||
nozzle_temperature = 270
|
||
nozzle_temperature_initial_layer = 270
|
||
slow_down_layer_time = 12
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 100
|
||
|
||
[filament:Bambu ASA-Aero @base]
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
filament_id = OGFB02
|
||
instantiation = false
|
||
description = This filament is only used to print models with a low density usually, and some special parameters are required. To get better printing quality, please refer to this wiki: ASA Aero Printing Guide.
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 50
|
||
fan_min_speed = 30
|
||
filament_cost = 49.99
|
||
filament_density = 0.99
|
||
filament_flow_ratio = 0.52
|
||
filament_max_volumetric_speed = 12
|
||
filament_retraction_length = 1.5
|
||
filament_type = ASA-AERO
|
||
filament_vendor = Bambu Lab
|
||
filament_wipe_distance = 5
|
||
filament_z_hop_types = Normal Lift
|
||
nozzle_temperature = 270
|
||
nozzle_temperature_initial_layer = 270
|
||
overhang_fan_speed = 50
|
||
reduce_fan_stop_start_freq = 0
|
||
slow_down_layer_time = 5
|
||
filament_scarf_seam_type = none
|
||
|
||
[filament:Bambu ASA-CF @base]
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
filament_id = OGFB51
|
||
instantiation = false
|
||
eng_plate_temp = 100
|
||
eng_plate_temp_initial_layer = 100
|
||
fan_max_speed = 25
|
||
filament_cost = 36.99
|
||
filament_density = 1.02
|
||
filament_flow_ratio = 0.9
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = ASA-CF
|
||
filament_vendor = Bambu Lab
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 100
|
||
nozzle_temperature = 275
|
||
nozzle_temperature_initial_layer = 275
|
||
nozzle_temperature_range_low = 250
|
||
slow_down_layer_time = 12
|
||
temperature_vitrification = 108
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 100
|
||
|
||
[filament:COEX ASA PRIME @base]
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
filament_id = CXASAB04
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 34.00
|
||
filament_density = 1.07
|
||
filament_type = ASA
|
||
filament_notes = UV and weather resistant - requires good ventilation
|
||
nozzle_temperature = 265
|
||
nozzle_temperature_initial_layer = 265
|
||
bed_temperature = 100
|
||
bed_temperature_initial_layer = 100
|
||
temperature_vitrification = 95
|
||
chamber_temperature = 0
|
||
filament_max_volumetric_speed = 16
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 2.5
|
||
filament_retraction_speed = 40
|
||
filament_deretraction_speed = 40
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 0
|
||
fan_max_speed = 30
|
||
disable_fan_first_layers = 3
|
||
full_fan_speed_layer = 0
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
enable_pressure_advance = 1
|
||
pressure_advance = 0.04
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:Elas ASA @base]
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
filament_id = OGFB01
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
activate_air_filtration = 0
|
||
activate_chamber_temp_control = 0
|
||
adaptive_pressure_advance = 0
|
||
adaptive_pressure_advance_bridges = 0
|
||
adaptive_pressure_advance_model = 0,0,0
|
||
0,0,0
|
||
adaptive_pressure_advance_overhangs = 0
|
||
additional_cooling_fan_speed = 0
|
||
chamber_temperature = 65
|
||
close_fan_the_first_x_layers = 3
|
||
complete_print_exhaust_fan_speed = 80
|
||
cool_plate_temp = 110
|
||
cool_plate_temp_initial_layer = 110
|
||
default_filament_colour =
|
||
dont_slow_down_outer_wall = 0
|
||
during_print_exhaust_fan_speed = 60
|
||
enable_overhang_bridge_fan = 1
|
||
enable_pressure_advance = 1
|
||
eng_plate_temp = 100
|
||
eng_plate_temp_initial_layer = 100
|
||
fan_cooling_layer_time = 35
|
||
fan_max_speed = 35
|
||
fan_min_speed = 10
|
||
filament_cooling_final_speed = 0
|
||
filament_cooling_initial_speed = 0
|
||
filament_cooling_moves = 0
|
||
filament_cost = 599
|
||
filament_density = 1.04
|
||
filament_deretraction_speed = nil
|
||
filament_diameter = 1.75
|
||
filament_flow_ratio = 0.95
|
||
filament_is_support = 0
|
||
filament_loading_speed = 0
|
||
filament_loading_speed_start = 0
|
||
filament_long_retractions_when_cut = nil
|
||
filament_max_volumetric_speed = 15
|
||
filament_minimal_purge_on_wipe_tower = 0
|
||
filament_multitool_ramming = 0
|
||
filament_multitool_ramming_flow = 10
|
||
filament_multitool_ramming_volume = 10
|
||
filament_notes =
|
||
filament_retract_before_wipe = nil
|
||
filament_retract_lift_above = nil
|
||
filament_retract_lift_below = nil
|
||
filament_retract_lift_enforce = nil
|
||
filament_retract_restart_extra = nil
|
||
filament_retract_when_changing_layer = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
filament_retraction_length = nil
|
||
filament_retraction_minimum_travel = nil
|
||
filament_retraction_speed = nil
|
||
filament_shrink = 100%
|
||
filament_shrinkage_compensation_z = 100%
|
||
filament_soluble = 0
|
||
filament_stamping_distance = 0
|
||
filament_stamping_loading_speed = 0
|
||
filament_toolchange_delay = 0
|
||
filament_unloading_speed = 0
|
||
filament_unloading_speed_start = 0
|
||
filament_vendor = Elas
|
||
filament_wipe = nil
|
||
filament_wipe_distance = nil
|
||
filament_z_hop = nil
|
||
filament_z_hop_types = nil
|
||
full_fan_speed_layer = 0
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 100
|
||
idle_temperature = 0
|
||
internal_bridge_fan_speed = -1
|
||
ironing_fan_speed = -1
|
||
nozzle_temperature = 270
|
||
nozzle_temperature_initial_layer = 270
|
||
nozzle_temperature_range_high = 280
|
||
nozzle_temperature_range_low = 240
|
||
overhang_fan_speed = 80
|
||
overhang_fan_threshold = 25%
|
||
pellet_flow_coefficient = 0.4157
|
||
pressure_advance = 0.075
|
||
reduce_fan_stop_start_freq = 1
|
||
required_nozzle_HRC = 0
|
||
slow_down_for_layer_cooling = 1
|
||
slow_down_layer_time = 12
|
||
slow_down_min_speed = 20
|
||
supertack_plate_temp = 35
|
||
supertack_plate_temp_initial_layer = 35
|
||
support_material_interface_fan_speed = -1
|
||
temperature_vitrification = 100
|
||
textured_cool_plate_temp = 40
|
||
textured_cool_plate_temp_initial_layer = 40
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 100
|
||
|
||
[filament:Elegoo ASA @base]
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
filament_id = OGFE06
|
||
instantiation = false
|
||
filament_vendor = Elegoo
|
||
filament_density = 1.1
|
||
filament_max_volumetric_speed = 12
|
||
|
||
[filament:Eolas Prints ASA @System]
|
||
filament_id = GFSEP018
|
||
setting_id = GFSEP018_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_asa
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = ASA
|
||
nozzle_temperature = 260
|
||
nozzle_temperature_initial_layer = 270
|
||
nozzle_temperature_range_low = 245
|
||
nozzle_temperature_range_high = 275
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 105
|
||
chamber_temperature = 40
|
||
filament_density = 1.07
|
||
filament_cost = 22.50
|
||
filament_spool_weight = 900
|
||
filament_max_volumetric_speed = 18
|
||
|
||
[filament:Generic ASA @System]
|
||
renamed_from = My Generic ASA
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFB98
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Overture ASA @base]
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
filament_id = GFOT009
|
||
instantiation = false
|
||
fan_cooling_layer_time = 45
|
||
fan_max_speed = 60
|
||
fan_min_speed = 10
|
||
filament_cost = 29.99
|
||
filament_density = 1.14
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 10
|
||
filament_vendor = Overture
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 100
|
||
nozzle_temperature = 270
|
||
nozzle_temperature_initial_layer = 270
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 240
|
||
slow_down_layer_time = 2
|
||
temperature_vitrification = 106
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 100
|
||
|
||
[filament:PolyLite ASA @base]
|
||
inherits = fdm_filament_asa
|
||
from = system
|
||
filament_id = OGFB61
|
||
instantiation = false
|
||
eng_plate_temp = 100
|
||
eng_plate_temp_initial_layer = 100
|
||
filament_cost = 23.6
|
||
filament_density = 1.02
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Polymaker
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 100
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 100
|
||
|
||
[filament:Generic BVOH @System]
|
||
inherits = fdm_filament_bvoh
|
||
from = system
|
||
setting_id = OGFSS97_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Generic CoPE @System]
|
||
inherits = fdm_filament_cope
|
||
from = system
|
||
setting_id = OGFSC99_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Generic EVA @System]
|
||
inherits = fdm_filament_eva
|
||
from = system
|
||
setting_id = OGFSR99_00
|
||
instantiation = true
|
||
description = This is neither a commonly used filament, nor one of Bambu filaments, and it varies a lot from brand to brand. So, it's highly recommended to ask its vendor for suitable profile before printing and adjust some parameters according to its performances.
|
||
compatible_printers =
|
||
|
||
[filament:FDplast HIPS @base]
|
||
inherits = fdm_filament_hips
|
||
from = system
|
||
filament_id = FDPLAST02
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 11
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = FDplast
|
||
nozzle_temperature = 250
|
||
nozzle_temperature_initial_layer = 250
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 250
|
||
hot_plate_temp = 110
|
||
hot_plate_temp_initial_layer = 110
|
||
textured_plate_temp = 110
|
||
textured_plate_temp_initial_layer = 110
|
||
|
||
[filament:Generic HIPS @System]
|
||
inherits = fdm_filament_hips
|
||
from = system
|
||
setting_id = OGFSS98_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:AliZ PA-CF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = AliZ003
|
||
instantiation = false
|
||
filament_type = PA-CF
|
||
complete_print_exhaust_fan_speed = 80
|
||
during_print_exhaust_fan_speed = 60
|
||
enable_pressure_advance = 0
|
||
eng_plate_temp = 80
|
||
eng_plate_temp_initial_layer = 80
|
||
fan_cooling_layer_time = 5
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 49.9
|
||
filament_flow_ratio = 1
|
||
filament_max_volumetric_speed = 8
|
||
filament_vendor = Aliz
|
||
full_fan_speed_layer = 2
|
||
nozzle_temperature = 290
|
||
nozzle_temperature_initial_layer = 290
|
||
nozzle_temperature_range_high = 300
|
||
nozzle_temperature_range_low = 260
|
||
overhang_fan_speed = 40
|
||
overhang_fan_threshold = 0%
|
||
pressure_advance = 0.026
|
||
slow_down_layer_time = 2
|
||
slow_down_min_speed = 10
|
||
|
||
[filament:Bambu PA-CF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFN03
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 84.99
|
||
filament_density = 1.09
|
||
filament_flow_ratio = 0.96
|
||
filament_type = PA-CF
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature = 280
|
||
nozzle_temperature_initial_layer = 280
|
||
overhang_fan_speed = 40
|
||
overhang_fan_threshold = 0%
|
||
temperature_vitrification = 170
|
||
|
||
[filament:Bambu PA6-CF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFN05
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
fan_cooling_layer_time = 5
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 79.99
|
||
filament_density = 1.10
|
||
filament_flow_ratio = 0.96
|
||
filament_type = PA6-CF
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature = 275
|
||
nozzle_temperature_initial_layer = 275
|
||
overhang_fan_speed = 40
|
||
overhang_fan_threshold = 0%
|
||
temperature_vitrification = 170
|
||
|
||
[filament:Bambu PA6-GF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFN08
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
fan_cooling_layer_time = 5
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 59.99
|
||
filament_density = 1.14
|
||
filament_flow_ratio = 0.96
|
||
filament_type = PA-GF
|
||
filament_vendor = Bambu Lab
|
||
full_fan_speed_layer = 2
|
||
overhang_fan_speed = 40
|
||
overhang_fan_threshold = 0%
|
||
temperature_vitrification = 180
|
||
|
||
[filament:Bambu PAHT-CF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFN04
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
fan_cooling_layer_time = 5
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 94.99
|
||
filament_density = 1.06
|
||
filament_flow_ratio = 0.96
|
||
filament_type = PA-CF
|
||
filament_vendor = Bambu Lab
|
||
full_fan_speed_layer = 2
|
||
overhang_fan_speed = 40
|
||
overhang_fan_threshold = 0%
|
||
temperature_vitrification = 180
|
||
|
||
[filament:Bambu Support For PA/PET @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFS03
|
||
instantiation = false
|
||
description = This is a non-water-soluble support filament, and usually it is only for the support structure and not for the model body. To get better printing quality, please refer to this wiki: Printing Tips for Support Filament and Support Function.
|
||
fan_cooling_layer_time = 10
|
||
filament_cost = 34.99
|
||
filament_density = 1.22
|
||
filament_is_support = 1
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature = 280
|
||
nozzle_temperature_initial_layer = 280
|
||
required_nozzle_HRC = 3
|
||
slow_down_layer_time = 6
|
||
|
||
[filament:Bambu Support G @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFS01
|
||
instantiation = false
|
||
description = This is a non-water-soluble support filament, and usually it is only for the support structure and not for the model body. To get better printing quality, please refer to this wiki: Printing Tips for Support Filament and Support Function.
|
||
fan_cooling_layer_time = 10
|
||
filament_cost = 34.99
|
||
filament_density = 1.22
|
||
filament_is_support = 1
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature = 280
|
||
nozzle_temperature_initial_layer = 280
|
||
required_nozzle_HRC = 3
|
||
filament_scarf_seam_type = none
|
||
slow_down_layer_time = 6
|
||
|
||
[filament:COEX NYLEX PA6-CF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = CXPACB23
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 85.00
|
||
filament_density = 1.24
|
||
filament_type = PA-CF
|
||
nozzle_temperature = 285
|
||
nozzle_temperature_initial_layer = 285
|
||
bed_temperature = 100
|
||
bed_temperature_initial_layer = 100
|
||
temperature_vitrification = 170
|
||
chamber_temperature = 60
|
||
filament_max_volumetric_speed = 11
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 2.5
|
||
filament_retraction_speed = 40
|
||
filament_deretraction_speed = 40
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 0
|
||
fan_max_speed = 30
|
||
disable_fan_first_layers = 4
|
||
full_fan_speed_layer = 0
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
enable_pressure_advance = 1
|
||
pressure_advance = 0.02
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:COEX NYLEX UNFILLED @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = CXPAUB21
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 85.00
|
||
filament_density = 1.08
|
||
filament_type = PA
|
||
nozzle_temperature = 260
|
||
nozzle_temperature_initial_layer = 260
|
||
bed_temperature = 100
|
||
bed_temperature_initial_layer = 100
|
||
temperature_vitrification = 100
|
||
chamber_temperature = 0
|
||
filament_max_volumetric_speed = 11
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 2.5
|
||
filament_retraction_speed = 40
|
||
filament_deretraction_speed = 40
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 0
|
||
fan_max_speed = 30
|
||
disable_fan_first_layers = 4
|
||
full_fan_speed_layer = 0
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
enable_pressure_advance = 1
|
||
pressure_advance = 0.02
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:Fiberon PA12-CF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFL52
|
||
instantiation = false
|
||
eng_plate_temp = 40
|
||
eng_plate_temp_initial_layer = 40
|
||
fan_cooling_layer_time = 15
|
||
fan_max_speed = 100
|
||
filament_cost = 99.99
|
||
filament_density = 1.06
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 14
|
||
filament_type = PA-CF
|
||
filament_vendor = Polymaker
|
||
full_fan_speed_layer = 2
|
||
hot_plate_temp = 40
|
||
hot_plate_temp_initial_layer = 40
|
||
nozzle_temperature = 300
|
||
nozzle_temperature_initial_layer = 300
|
||
nozzle_temperature_range_low = 260
|
||
overhang_fan_speed = 100
|
||
reduce_fan_stop_start_freq = 1
|
||
temperature_vitrification = 131
|
||
textured_plate_temp = 40
|
||
textured_plate_temp_initial_layer = 40
|
||
|
||
[filament:Fiberon PA6-CF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFL50
|
||
instantiation = false
|
||
eng_plate_temp = 40
|
||
eng_plate_temp_initial_layer = 40
|
||
fan_cooling_layer_time = 15
|
||
fan_max_speed = 100
|
||
filament_cost = 83.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PA6-CF
|
||
filament_vendor = Polymaker
|
||
hot_plate_temp = 40
|
||
hot_plate_temp_initial_layer = 40
|
||
nozzle_temperature = 300
|
||
nozzle_temperature_initial_layer = 300
|
||
nozzle_temperature_range_low = 280
|
||
overhang_fan_speed = 100
|
||
reduce_fan_stop_start_freq = 1
|
||
temperature_vitrification = 215
|
||
textured_plate_temp = 40
|
||
textured_plate_temp_initial_layer = 40
|
||
|
||
[filament:Fiberon PA6-GF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFL51
|
||
instantiation = false
|
||
eng_plate_temp = 40
|
||
eng_plate_temp_initial_layer = 40
|
||
fan_cooling_layer_time = 15
|
||
fan_max_speed = 100
|
||
filament_cost = 63.99
|
||
filament_density = 1.2
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PA-GF
|
||
filament_vendor = Polymaker
|
||
full_fan_speed_layer = 2
|
||
hot_plate_temp = 40
|
||
hot_plate_temp_initial_layer = 40
|
||
nozzle_temperature = 300
|
||
nozzle_temperature_initial_layer = 300
|
||
nozzle_temperature_range_low = 280
|
||
overhang_fan_speed = 100
|
||
reduce_fan_stop_start_freq = 1
|
||
temperature_vitrification = 191
|
||
textured_plate_temp = 40
|
||
textured_plate_temp_initial_layer = 40
|
||
|
||
[filament:Fiberon PA612-CF @base]
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
filament_id = OGFL53
|
||
instantiation = false
|
||
fan_cooling_layer_time = 5
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 94.99
|
||
filament_density = 1.06
|
||
filament_flow_ratio = 0.96
|
||
filament_vendor = Polymaker
|
||
full_fan_speed_layer = 2
|
||
overhang_fan_speed = 40
|
||
overhang_fan_threshold = 0%
|
||
temperature_vitrification = 180
|
||
|
||
[filament:Generic PA @System]
|
||
renamed_from = My Generic PA
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFN99
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Generic PA-CF @System]
|
||
renamed_from = My Generic PA-CF
|
||
inherits = fdm_filament_pa
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFN98
|
||
instantiation = true
|
||
filament_type = PA-CF
|
||
compatible_printers =
|
||
|
||
[filament:Elegoo PAHT @base]
|
||
inherits = fdm_filament_paht
|
||
from = system
|
||
filament_id = EPAHTB00
|
||
instantiation = false
|
||
filament_cost = 0
|
||
filament_density = 1.25
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Elegoo
|
||
filament_start_gcode = ; filament start gcode
|
||
|
||
[filament:Bambu PC @base]
|
||
inherits = fdm_filament_pc
|
||
from = system
|
||
filament_id = OGFC00
|
||
instantiation = false
|
||
filament_vendor = Bambu Lab
|
||
filament_cost = 39.99
|
||
filament_flow_ratio = 0.94
|
||
|
||
[filament:Bambu PC FR @base]
|
||
inherits = fdm_filament_pc
|
||
from = system
|
||
filament_id = OGFC01
|
||
instantiation = false
|
||
filament_cost = 0
|
||
filament_density = 1.19
|
||
filament_flow_ratio = 0.94
|
||
filament_vendor = Bambu Lab
|
||
|
||
[filament:Elegoo PC @base]
|
||
inherits = fdm_filament_pc
|
||
from = system
|
||
filament_id = EPCB00
|
||
instantiation = false
|
||
filament_cost = 0
|
||
filament_density = 1.25
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Elegoo
|
||
filament_start_gcode = ; filament start gcode
|
||
|
||
[filament:Generic PC @System]
|
||
renamed_from = My Generic PC
|
||
inherits = fdm_filament_pc
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFC99
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:COEX PCTG PRIME @base]
|
||
inherits = fdm_filament_pctg
|
||
from = system
|
||
filament_id = CXPCTB15
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 38.00
|
||
filament_density = 1.27
|
||
filament_type = PCTG
|
||
filament_notes = High clarity and chemical resistance copolyester
|
||
nozzle_temperature = 275
|
||
nozzle_temperature_initial_layer = 275
|
||
bed_temperature = 80
|
||
bed_temperature_initial_layer = 85
|
||
temperature_vitrification = 80
|
||
filament_max_volumetric_speed = 12
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 3.5
|
||
filament_retraction_speed = 35
|
||
filament_deretraction_speed = 35
|
||
filament_z_hop = 0.4
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 30
|
||
fan_max_speed = 50
|
||
disable_fan_first_layers = 2
|
||
full_fan_speed_layer = 4
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
enable_pressure_advance = 1
|
||
pressure_advance = 0.045
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:Generic PCTG @System]
|
||
inherits = fdm_filament_pctg
|
||
from = system
|
||
setting_id = OGFSG97_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Generic PE @System]
|
||
inherits = fdm_filament_pe
|
||
from = system
|
||
setting_id = OGFSP99_00
|
||
instantiation = true
|
||
description = This is neither a commonly used filament, nor one of Bambu filaments, and it varies a lot from brand to brand. So, it's highly recommended to ask its vendor for suitable profile before printing and adjust some parameters according to its performances.
|
||
compatible_printers =
|
||
|
||
[filament:Generic PE-CF @System]
|
||
inherits = fdm_filament_pe
|
||
from = system
|
||
setting_id = OGFSP98_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:AliZ PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = AliZ001
|
||
instantiation = false
|
||
close_fan_the_first_x_layers = 2
|
||
enable_pressure_advance = 0
|
||
fan_max_speed = 80
|
||
fan_min_speed = 30
|
||
filament_cost = 49.9
|
||
filament_flow_ratio = 1
|
||
filament_max_volumetric_speed = 15
|
||
filament_vendor = Aliz
|
||
hot_plate_temp = 79
|
||
hot_plate_temp_initial_layer = 79
|
||
nozzle_temperature = 250
|
||
nozzle_temperature_initial_layer = 250
|
||
overhang_fan_threshold = 25%
|
||
pressure_advance = 0.036
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:Bambu PET-CF @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFT01
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 80
|
||
eng_plate_temp_initial_layer = 80
|
||
fan_cooling_layer_time = 5
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 84.99
|
||
filament_density = 1.29
|
||
filament_max_volumetric_speed = 8
|
||
filament_type = PET-CF
|
||
filament_vendor = Bambu Lab
|
||
hot_plate_temp = 100
|
||
hot_plate_temp_initial_layer = 100
|
||
nozzle_temperature = 270
|
||
nozzle_temperature_initial_layer = 270
|
||
nozzle_temperature_range_high = 290
|
||
nozzle_temperature_range_low = 260
|
||
overhang_fan_speed = 40
|
||
overhang_fan_threshold = 0%
|
||
required_nozzle_HRC = 40
|
||
supertack_plate_temp = 80
|
||
supertack_plate_temp_initial_layer = 80
|
||
slow_down_layer_time = 2
|
||
temperature_vitrification = 185
|
||
textured_plate_temp = 100
|
||
textured_plate_temp_initial_layer = 100
|
||
|
||
[filament:Bambu PETG Basic @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFG00
|
||
instantiation = false
|
||
description = To get better transparent or translucent results with the corresponding filament, please refer to this wiki: Printing tips for transparent PETG.
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 40
|
||
fan_min_speed = 10
|
||
filament_cost = 24.99
|
||
filament_density = 1.25
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 8
|
||
filament_vendor = Bambu Lab
|
||
hot_plate_temp = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 230
|
||
overhang_fan_speed = 90
|
||
overhang_fan_threshold = 10%
|
||
slow_down_layer_time = 12
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:Bambu PETG HF @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFG02
|
||
instantiation = false
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 40
|
||
fan_min_speed = 10
|
||
filament_cost = 24.99
|
||
filament_density = 1.28
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Bambu Lab
|
||
hot_plate_temp = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
nozzle_temperature = 245
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 230
|
||
overhang_fan_speed = 90
|
||
overhang_fan_threshold = 10%
|
||
slow_down_layer_time = 12
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:Bambu PETG Translucent @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFG01
|
||
instantiation = false
|
||
description = To get better transparent or translucent results with the corresponding filament, please refer to this wiki: Printing tips for transparent PETG.
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 24.99
|
||
filament_density = 1.25
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 6
|
||
filament_vendor = Bambu Lab
|
||
hot_plate_temp = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
nozzle_temperature = 245
|
||
nozzle_temperature_initial_layer = 250
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 230
|
||
overhang_fan_speed = 90
|
||
overhang_fan_threshold = 10%
|
||
slow_down_layer_time = 12
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:Bambu PETG-CF @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFG50
|
||
instantiation = false
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
fan_max_speed = 30
|
||
fan_min_speed = 0
|
||
filament_cost = 34.99
|
||
filament_density = 1.25
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PETG-CF
|
||
filament_vendor = Bambu Lab
|
||
hot_plate_temp = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 240
|
||
overhang_fan_speed = 90
|
||
overhang_fan_threshold = 10%
|
||
required_nozzle_HRC = 40
|
||
slow_down_layer_time = 6
|
||
temperature_vitrification = 70
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:COEX PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = CXPETB13
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 33.00
|
||
filament_density = 1.27
|
||
filament_type = PETG
|
||
filament_notes = IMPORTANT: Set travel speed to maximum your machine allows (200-500mm/s) to reduce stringing
|
||
nozzle_temperature = 245
|
||
nozzle_temperature_initial_layer = 250
|
||
bed_temperature = 80
|
||
bed_temperature_initial_layer = 85
|
||
temperature_vitrification = 70
|
||
filament_max_volumetric_speed = 12
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 4
|
||
filament_retraction_speed = 30
|
||
filament_deretraction_speed = 30
|
||
filament_z_hop = 0.4
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 30
|
||
fan_max_speed = 50
|
||
disable_fan_first_layers = 2
|
||
full_fan_speed_layer = 4
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
enable_pressure_advance = 1
|
||
pressure_advance = 0.045
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:Elas PETG Basic @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFG00
|
||
instantiation = false
|
||
description = To get better transparent or translucent results with the corresponding filament, please refer to this wiki: Printing tips for transparent PETG.
|
||
complete_print_exhaust_fan_speed = 80
|
||
cool_plate_temp = 60
|
||
cool_plate_temp_initial_layer = 60
|
||
dont_slow_down_outer_wall = 0
|
||
during_print_exhaust_fan_speed = 60
|
||
enable_overhang_bridge_fan = 1
|
||
enable_pressure_advance = 1
|
||
eng_plate_temp = 80
|
||
eng_plate_temp_initial_layer = 80
|
||
fan_cooling_layer_time = 20
|
||
fan_max_speed = 100
|
||
fan_min_speed = 20
|
||
filament_cooling_final_speed = 0
|
||
filament_cooling_initial_speed = 0
|
||
filament_cooling_moves = 0
|
||
filament_cost = 445
|
||
filament_density = 1.27
|
||
filament_deretraction_speed = nil
|
||
filament_diameter = 1.75
|
||
filament_flow_ratio = 1
|
||
filament_is_support = 0
|
||
filament_loading_speed = 0
|
||
filament_loading_speed_start = 0
|
||
filament_long_retractions_when_cut = 1
|
||
filament_max_volumetric_speed = 18
|
||
filament_minimal_purge_on_wipe_tower = 0
|
||
filament_multitool_ramming = 0
|
||
filament_multitool_ramming_flow = 10
|
||
filament_multitool_ramming_volume = 10
|
||
filament_notes =
|
||
filament_retract_before_wipe = nil
|
||
filament_retract_lift_above = nil
|
||
filament_retract_lift_below = nil
|
||
filament_retract_lift_enforce = nil
|
||
filament_retract_restart_extra = nil
|
||
filament_retract_when_changing_layer = nil
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_retraction_length = nil
|
||
filament_retraction_minimum_travel = nil
|
||
filament_retraction_speed = nil
|
||
filament_shrink = 99.7%
|
||
filament_shrinkage_compensation_z = 100%
|
||
filament_soluble = 0
|
||
filament_stamping_distance = 0
|
||
filament_stamping_loading_speed = 0
|
||
filament_toolchange_delay = 0
|
||
filament_unloading_speed = 0
|
||
filament_unloading_speed_start = 0
|
||
filament_wipe = nil
|
||
filament_wipe_distance = nil
|
||
filament_z_hop = nil
|
||
filament_z_hop_types = nil
|
||
full_fan_speed_layer = 0
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 80
|
||
idle_temperature = 0
|
||
internal_bridge_fan_speed = -1
|
||
ironing_fan_speed = -1
|
||
filament_vendor = Elas
|
||
nozzle_temperature = 250
|
||
nozzle_temperature_initial_layer = 245
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 230
|
||
overhang_fan_speed = 100
|
||
overhang_fan_threshold = 10%
|
||
pellet_flow_coefficient = 0.4157
|
||
pressure_advance = 0.035
|
||
reduce_fan_stop_start_freq = 1
|
||
required_nozzle_HRC = 3
|
||
slow_down_for_layer_cooling = 1
|
||
slow_down_layer_time = 8
|
||
slow_down_min_speed = 10
|
||
supertack_plate_temp = 70
|
||
supertack_plate_temp_initial_layer = 70
|
||
support_material_interface_fan_speed = -1
|
||
temperature_vitrification = 70
|
||
textured_cool_plate_temp = 40
|
||
textured_cool_plate_temp_initial_layer = 40
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 80
|
||
|
||
[filament:Elegoo PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = EPETGB00
|
||
instantiation = false
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 40
|
||
fan_min_speed = 10
|
||
filament_cost = 0
|
||
filament_density = 1.25
|
||
filament_max_volumetric_speed = 8
|
||
filament_vendor = Elegoo
|
||
hot_plate_temp = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 230
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 240
|
||
overhang_fan_speed = 90
|
||
overhang_fan_threshold = 10%
|
||
slow_down_layer_time = 12
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
filament_start_gcode = ; Filament start gcode
|
||
|
||
filament_end_gcode = ; filament end gcode
|
||
|
||
filament_type = PETG
|
||
|
||
[filament:Elegoo PETG PRO @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFE02
|
||
instantiation = false
|
||
filament_cost = 12.49
|
||
filament_density = 1.27
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_retraction_length = 0.8
|
||
filament_retraction_speed = 45
|
||
filament_deretraction_speed = 45
|
||
filament_vendor = Elegoo
|
||
nozzle_temperature = 245
|
||
nozzle_temperature_initial_layer = 240
|
||
nozzle_temperature_range_high = 260
|
||
nozzle_temperature_range_low = 230
|
||
hot_plate_temp = 65
|
||
hot_plate_temp_initial_layer = 65
|
||
textured_plate_temp = 75
|
||
textured_plate_temp_initial_layer = 75
|
||
overhang_fan_speed = 90
|
||
fan_max_speed = 80
|
||
fan_min_speed = 20
|
||
fan_cooling_layer_time = 20
|
||
slow_down_layer_time = 10
|
||
slow_down_min_speed = 20
|
||
|
||
[filament:Elegoo PETG-CF @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFE03
|
||
instantiation = false
|
||
filament_cost = 18.99
|
||
filament_density = 1.29
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 10
|
||
filament_retraction_length = 0.8
|
||
filament_retraction_speed = 45
|
||
filament_deretraction_speed = 45
|
||
filament_vendor = Elegoo
|
||
nozzle_temperature = 255
|
||
nozzle_temperature_initial_layer = 250
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 240
|
||
hot_plate_temp = 65
|
||
hot_plate_temp_initial_layer = 65
|
||
textured_plate_temp = 75
|
||
textured_plate_temp_initial_layer = 75
|
||
overhang_fan_speed = 90
|
||
fan_max_speed = 80
|
||
fan_min_speed = 20
|
||
fan_cooling_layer_time = 20
|
||
slow_down_layer_time = 10
|
||
slow_down_min_speed = 20
|
||
|
||
[filament:Elegoo Rapid PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFE01
|
||
instantiation = false
|
||
filament_cost = 13.99
|
||
filament_density = 1.28
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 20
|
||
filament_retraction_length = 0.8
|
||
filament_retraction_speed = 45
|
||
filament_deretraction_speed = 45
|
||
filament_vendor = Elegoo
|
||
nozzle_temperature = 255
|
||
nozzle_temperature_initial_layer = 250
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 240
|
||
hot_plate_temp = 65
|
||
hot_plate_temp_initial_layer = 65
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
overhang_fan_speed = 90
|
||
fan_max_speed = 80
|
||
fan_min_speed = 20
|
||
fan_cooling_layer_time = 20
|
||
slow_down_layer_time = 10
|
||
slow_down_min_speed = 20
|
||
|
||
[filament:Eolas Prints PETG @System]
|
||
filament_id = GFSEP010
|
||
setting_id = GFSEP010_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pet
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PETG
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 245
|
||
nozzle_temperature_range_low = 230
|
||
nozzle_temperature_range_high = 260
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 85
|
||
filament_density = 1.27
|
||
filament_cost = 25.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:Eolas Prints PETG Transition @System]
|
||
filament_id = GFSEP012
|
||
setting_id = GFSEP012_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pet
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PETG
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 245
|
||
nozzle_temperature_range_low = 230
|
||
nozzle_temperature_range_high = 260
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 85
|
||
filament_density = 1.27
|
||
filament_cost = 17.40
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:Eolas Prints PETG UV Resistant @System]
|
||
filament_id = GFSEP011
|
||
setting_id = GFSEP011_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pet
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PETG
|
||
nozzle_temperature = 245
|
||
nozzle_temperature_initial_layer = 250
|
||
nozzle_temperature_range_low = 235
|
||
nozzle_temperature_range_high = 265
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 85
|
||
filament_density = 1.27
|
||
filament_cost = 30.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:FDplast PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = FDPLAST03
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 11
|
||
default_filament_colour =
|
||
filament_vendor = FDplast
|
||
filament_density = 1.27
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 20
|
||
fan_max_speed = 100
|
||
fan_min_speed = 30
|
||
nozzle_temperature = 235
|
||
nozzle_temperature_initial_layer = 240
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 220
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 80
|
||
textured_plate_temp = 80
|
||
textured_plate_temp_initial_layer = 80
|
||
compatible_printers =
|
||
|
||
[filament:Fiberon PET-CF @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFL54
|
||
instantiation = false
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
fan_cooling_layer_time = 242
|
||
fan_min_speed = 0
|
||
filament_cost = 89.99
|
||
filament_density = 1.34
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PET-CF
|
||
filament_vendor = Polymaker
|
||
hot_plate_temp = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
nozzle_temperature = 300
|
||
nozzle_temperature_initial_layer = 300
|
||
nozzle_temperature_range_high = 300
|
||
nozzle_temperature_range_low = 270
|
||
required_nozzle_HRC = 40
|
||
supertack_plate_temp = 80
|
||
supertack_plate_temp_initial_layer = 80
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 147
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:Fiberon PETG-ESD @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFL06
|
||
instantiation = false
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 60
|
||
eng_plate_temp_initial_layer = 60
|
||
fan_cooling_layer_time = 15
|
||
fan_min_speed = 0
|
||
filament_cost = 0
|
||
filament_density = 1.24
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Polymaker
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
nozzle_temperature = 290
|
||
nozzle_temperature_initial_layer = 290
|
||
nozzle_temperature_range_high = 290
|
||
nozzle_temperature_range_low = 250
|
||
slow_down_layer_time = 2
|
||
slow_down_min_speed = 10
|
||
temperature_vitrification = 76
|
||
textured_plate_temp = 60
|
||
textured_plate_temp_initial_layer = 60
|
||
|
||
[filament:Fiberon PETG-rCF @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFL55
|
||
instantiation = false
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
fan_cooling_layer_time = 12
|
||
fan_min_speed = 0
|
||
filament_cost = 39.99
|
||
filament_density = 1.3
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_type = PETG-CF
|
||
filament_vendor = Polymaker
|
||
hot_plate_temp = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
nozzle_temperature = 270
|
||
nozzle_temperature_initial_layer = 270
|
||
nozzle_temperature_range_high = 270
|
||
nozzle_temperature_range_low = 240
|
||
required_nozzle_HRC = 40
|
||
slow_down_layer_time = 2
|
||
slow_down_min_speed = 10
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:Generic PETG @System]
|
||
renamed_from = My Generic PETG
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFG99
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Generic PETG HF @System]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
setting_id = OGFSG96_00
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 20
|
||
compatible_printers =
|
||
|
||
[filament:Generic PETG-CF @System]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
setting_id = OGFSG50
|
||
instantiation = true
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 40
|
||
fan_min_speed = 5
|
||
filament_max_volumetric_speed = 11.5
|
||
overhang_fan_speed = 100
|
||
compatible_printers =
|
||
|
||
[filament:NIT PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = NIT03
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 12
|
||
default_filament_colour =
|
||
filament_vendor = NIT
|
||
filament_density = 1.27
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 20
|
||
fan_max_speed = 100
|
||
fan_min_speed = 30
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 245
|
||
nozzle_temperature_range_high = 250
|
||
nozzle_temperature_range_low = 230
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 80
|
||
textured_plate_temp = 80
|
||
textured_plate_temp_initial_layer = 80
|
||
compatible_printers =
|
||
|
||
[filament:PolyLite PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFG60
|
||
instantiation = false
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 70
|
||
eng_plate_temp_initial_layer = 70
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 90
|
||
fan_min_speed = 40
|
||
filament_flow_ratio = 0.95
|
||
filament_vendor = Polymaker
|
||
hot_plate_temp = 70
|
||
hot_plate_temp_initial_layer = 70
|
||
overhang_fan_speed = 90
|
||
overhang_fan_threshold = 10%
|
||
slow_down_layer_time = 12
|
||
slow_down_min_speed = 10
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:SUNLU PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = OGFSNL08
|
||
instantiation = false
|
||
description = To get better transparent or translucent results with the corresponding filament, please refer to this wiki: Printing tips for transparent PETG.
|
||
cool_plate_temp = 0
|
||
cool_plate_temp_initial_layer = 0
|
||
eng_plate_temp = 60
|
||
eng_plate_temp_initial_layer = 60
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
filament_cost = 22.99
|
||
filament_density = 1.27
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = SUNLU
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
nozzle_temperature = 245
|
||
nozzle_temperature_initial_layer = 250
|
||
nozzle_temperature_range_high = 280
|
||
nozzle_temperature_range_low = 230
|
||
overhang_fan_speed = 90
|
||
overhang_fan_threshold = 10%
|
||
slow_down_layer_time = 12
|
||
textured_plate_temp = 60
|
||
textured_plate_temp_initial_layer = 60
|
||
temperature_vitrification = 68
|
||
|
||
[filament:eSUN PETG @base]
|
||
inherits = fdm_filament_pet
|
||
from = system
|
||
filament_id = ESN03
|
||
instantiation = false
|
||
filament_vendor = eSUN
|
||
filament_density = 1.27
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 10
|
||
fan_max_speed = 100
|
||
fan_min_speed = 30
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 240
|
||
nozzle_temperature_range_high = 250
|
||
nozzle_temperature_range_low = 230
|
||
temperature_vitrification = 64
|
||
hot_plate_temp = 65
|
||
hot_plate_temp_initial_layer = 65
|
||
textured_plate_temp = 65
|
||
textured_plate_temp_initial_layer = 65
|
||
compatible_printers =
|
||
|
||
[filament:Generic PHA @System]
|
||
inherits = fdm_filament_pha
|
||
from = system
|
||
setting_id = OGFSR98_00
|
||
instantiation = true
|
||
description = This is neither a commonly used filament, nor one of Bambu filaments, and it varies a lot from brand to brand. So, it's highly recommended to ask its vendor for suitable profile before printing and adjust some parameters according to its performances.
|
||
compatible_printers =
|
||
|
||
[filament:AliZ PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = AliZ002
|
||
instantiation = false
|
||
enable_pressure_advance = 0
|
||
fan_cooling_layer_time = 100
|
||
filament_cost = 69
|
||
filament_density = 1.27
|
||
filament_vendor = Aliz
|
||
filament_wipe_distance = 0
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
pressure_advance = 0.025
|
||
slow_down_layer_time = 4
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
|
||
[filament:Bambu PLA Aero @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA11
|
||
instantiation = false
|
||
description = This filament is only used to print models with a low density usually, and some special parameters are required. To get better printing quality, please refer to this wiki: Instructions for printing RC model with foaming PLA (PLA Aero).
|
||
fan_min_speed = 30
|
||
filament_cost = 44.99
|
||
filament_density = 1.21
|
||
filament_flow_ratio = 0.6
|
||
filament_max_volumetric_speed = 6
|
||
filament_type = PLA-AERO
|
||
filament_vendor = Bambu Lab
|
||
filament_scarf_seam_type = none
|
||
nozzle_temperature_range_low = 210
|
||
nozzle_temperature_range_high = 260
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
|
||
[filament:Bambu PLA Basic @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA00
|
||
instantiation = false
|
||
filament_cost = 24.99
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Bambu Lab
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_height = 10%
|
||
filament_scarf_gap = 0%
|
||
filament_scarf_length = 10
|
||
|
||
[filament:Bambu PLA Dynamic @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA13
|
||
instantiation = false
|
||
filament_cost = 31.99
|
||
filament_density = 1.26
|
||
filament_vendor = Bambu Lab
|
||
|
||
[filament:Bambu PLA Galaxy @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA15
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.19
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Bambu Lab
|
||
|
||
[filament:Bambu PLA Glow @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA12
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Bambu Lab
|
||
temperature_vitrification = 45
|
||
|
||
[filament:Bambu PLA Impact @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA03
|
||
instantiation = false
|
||
filament_cost = 25.4
|
||
filament_flow_ratio = 0.95
|
||
filament_vendor = Bambu Lab
|
||
|
||
[filament:Bambu PLA Marble @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA07
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.22
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Bambu Lab
|
||
|
||
[filament:Bambu PLA Matte @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA01
|
||
instantiation = false
|
||
filament_cost = 24.99
|
||
filament_density = 1.32
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Bambu Lab
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_height = 5%
|
||
filament_scarf_gap = 0%
|
||
filament_scarf_length = 10
|
||
|
||
[filament:Bambu PLA Metal @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA02
|
||
instantiation = false
|
||
description = To make the prints get higher gloss, please dry the filament before use, and set the outer wall speed to be 40 to 60 mm/s when slicing.
|
||
filament_cost = 29.99
|
||
filament_density = 1.25
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Bambu Lab
|
||
filament_scarf_seam_type = none
|
||
|
||
[filament:Bambu PLA Silk @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA05
|
||
instantiation = false
|
||
description = To make the prints get higher gloss, please dry the filament before use, and set the outer wall speed to be 40 to 60 mm/s when slicing.
|
||
filament_cost = 29.99
|
||
filament_density = 1.32
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Bambu Lab
|
||
filament_scarf_height = 5%
|
||
filament_scarf_gap = 0%
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
|
||
[filament:Bambu PLA Silk+ @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA06
|
||
instantiation = false
|
||
description = To make the prints get higher gloss, please dry the filament before use, and set the outer wall speed to be 40 to 60 mm/s when slicing.
|
||
filament_cost = 29.99
|
||
filament_density = 1.27
|
||
filament_flow_ratio = 0.98
|
||
filament_scarf_height = 5%
|
||
filament_scarf_seam_type = all
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
|
||
[filament:Bambu PLA Sparkle @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA08
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Bambu Lab
|
||
|
||
[filament:Bambu PLA Tough @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA09
|
||
instantiation = false
|
||
filament_cost = 28.99
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Bambu Lab
|
||
filament_scarf_seam_type = none
|
||
|
||
[filament:Bambu PLA Wood @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA16
|
||
instantiation = false
|
||
filament_cost = 24.99
|
||
filament_density = 1.21
|
||
filament_flow_ratio = 0.98
|
||
filament_long_retractions_when_cut = 1
|
||
filament_max_volumetric_speed = 12
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_scarf_seam_type = none
|
||
filament_vendor = Bambu Lab
|
||
|
||
[filament:Bambu PLA-CF @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA50
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 0
|
||
cool_plate_temp = 45
|
||
cool_plate_temp_initial_layer = 45
|
||
filament_cost = 34.99
|
||
filament_density = 1.22
|
||
filament_flow_ratio = 0.98
|
||
filament_type = PLA-CF
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature_range_low = 210
|
||
nozzle_temperature_range_high = 250
|
||
required_nozzle_HRC = 40
|
||
supertack_plate_temp = 50
|
||
supertack_plate_temp_initial_layer = 50
|
||
slow_down_layer_time = 8
|
||
|
||
[filament:Bambu Support For PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFS02
|
||
instantiation = false
|
||
description = This is a non-water-soluble support filament, and usually it is only for the support structure and not for the model body. To get better printing quality, please refer to this wiki: Printing Tips for Support Filament and Support Function.
|
||
cool_plate_temp = 40
|
||
cool_plate_temp_initial_layer = 40
|
||
filament_cost = 69.98
|
||
filament_density = 1.30
|
||
filament_is_support = 1
|
||
filament_vendor = Bambu Lab
|
||
filament_scarf_seam_type = none
|
||
slow_down_layer_time = 8
|
||
|
||
[filament:Bambu Support For PLA/PETG @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFS05
|
||
instantiation = false
|
||
description = This is a non-water-soluble support filament, and usually it is only for the support structure and not for the model body. To get better printing quality, please refer to this wiki: Printing Tips for Support Filament and Support Function.
|
||
fan_cooling_layer_time = 80
|
||
fan_max_speed = 30
|
||
fan_min_speed = 20
|
||
filament_cost = 69.98
|
||
filament_density = 1.19
|
||
filament_is_support = 1
|
||
filament_max_volumetric_speed = 6
|
||
filament_scarf_seam_type = none
|
||
filament_vendor = Bambu Lab
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
nozzle_temperature = 210
|
||
nozzle_temperature_initial_layer = 210
|
||
slow_down_layer_time = 8
|
||
supertack_plate_temp_initial_layer = 0
|
||
textured_plate_temp = 60
|
||
textured_plate_temp_initial_layer = 60
|
||
|
||
[filament:Bambu Support W @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFS00
|
||
instantiation = false
|
||
description = This is a non-water-soluble support filament, and usually it is only for the support structure and not for the model body. To get better printing quality, please refer to this wiki: Printing Tips for Support Filament and Support Function.
|
||
cool_plate_temp = 40
|
||
cool_plate_temp_initial_layer = 40
|
||
filament_cost = 69.98
|
||
filament_density = 1.30
|
||
filament_is_support = 1
|
||
filament_vendor = Bambu Lab
|
||
filament_scarf_seam_type = none
|
||
slow_down_layer_time = 8
|
||
|
||
[filament:COEX PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = CXPLAB02
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 24.00
|
||
filament_density = 1.24
|
||
filament_type = PLA
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 235
|
||
bed_temperature = 60
|
||
bed_temperature_initial_layer = 60
|
||
temperature_vitrification = 55
|
||
filament_max_volumetric_speed = 18
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 1.5
|
||
filament_retraction_speed = 45
|
||
filament_deretraction_speed = 40
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 100
|
||
fan_max_speed = 100
|
||
disable_fan_first_layers = 1
|
||
full_fan_speed_layer = 3
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:COEX PLA PRIME @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = CXPLAB08
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 32.00
|
||
filament_density = 1.24
|
||
filament_type = PLA
|
||
filament_notes = Made with NatureWorks Ingeo 3D850 - improved heat resistance and toughness
|
||
nozzle_temperature = 235
|
||
nozzle_temperature_initial_layer = 240
|
||
bed_temperature = 60
|
||
bed_temperature_initial_layer = 60
|
||
temperature_vitrification = 60
|
||
filament_max_volumetric_speed = 15
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 1.2
|
||
filament_retraction_speed = 50
|
||
filament_deretraction_speed = 40
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 100
|
||
fan_max_speed = 100
|
||
disable_fan_first_layers = 1
|
||
full_fan_speed_layer = 3
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:Elas PLA Basic @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA00
|
||
instantiation = false
|
||
activate_air_filtration = 0
|
||
activate_chamber_temp_control = 0
|
||
adaptive_pressure_advance = 0
|
||
adaptive_pressure_advance_bridges = 0
|
||
adaptive_pressure_advance_model = 0,0,0
|
||
0,0,0
|
||
adaptive_pressure_advance_overhangs = 0
|
||
additional_cooling_fan_speed = 70
|
||
chamber_temperature = 0
|
||
close_fan_the_first_x_layers = 1
|
||
complete_print_exhaust_fan_speed = 70
|
||
cool_plate_temp = 35
|
||
cool_plate_temp_initial_layer = 35
|
||
default_filament_colour =
|
||
dont_slow_down_outer_wall = 0
|
||
during_print_exhaust_fan_speed = 70
|
||
enable_overhang_bridge_fan = 1
|
||
enable_pressure_advance = 1
|
||
eng_plate_temp = 55
|
||
eng_plate_temp_initial_layer = 55
|
||
fan_cooling_layer_time = 100
|
||
fan_max_speed = 80
|
||
fan_min_speed = 60
|
||
filament_cooling_final_speed = 0
|
||
filament_cooling_initial_speed = 0
|
||
filament_cooling_moves = 0
|
||
filament_cost = 449.5
|
||
filament_density = 1.24
|
||
filament_deretraction_speed = nil
|
||
filament_diameter = 1.75
|
||
filament_flow_ratio = 0.98
|
||
filament_is_support = 0
|
||
filament_loading_speed = 0
|
||
filament_loading_speed_start = 0
|
||
filament_long_retractions_when_cut = nil
|
||
filament_max_volumetric_speed = 25
|
||
filament_minimal_purge_on_wipe_tower = 0
|
||
filament_multitool_ramming = 0
|
||
filament_multitool_ramming_flow = 10
|
||
filament_multitool_ramming_volume = 10
|
||
filament_notes =
|
||
filament_retract_before_wipe = nil
|
||
filament_retract_lift_above = nil
|
||
filament_retract_lift_below = nil
|
||
filament_retract_lift_enforce = nil
|
||
filament_retract_restart_extra = nil
|
||
filament_retract_when_changing_layer = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
filament_retraction_length = nil
|
||
filament_retraction_minimum_travel = nil
|
||
filament_retraction_speed = nil
|
||
filament_shrink = 100%
|
||
filament_shrinkage_compensation_z = 100%
|
||
filament_soluble = 0
|
||
filament_stamping_distance = 0
|
||
filament_stamping_loading_speed = 0
|
||
filament_toolchange_delay = 0
|
||
filament_unloading_speed = 0
|
||
filament_unloading_speed_start = 0
|
||
filament_vendor = Elas
|
||
filament_wipe = nil
|
||
filament_wipe_distance = nil
|
||
filament_z_hop = nil
|
||
filament_z_hop_types = nil
|
||
full_fan_speed_layer = 0
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
idle_temperature = 0
|
||
internal_bridge_fan_speed = -1
|
||
ironing_fan_speed = -1
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
overhang_fan_speed = 100
|
||
overhang_fan_threshold = 50%
|
||
pellet_flow_coefficient = 0.4157
|
||
pressure_advance = 0.025
|
||
reduce_fan_stop_start_freq = 1
|
||
required_nozzle_HRC = 3
|
||
slow_down_for_layer_cooling = 1
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 20
|
||
supertack_plate_temp = 45
|
||
supertack_plate_temp_initial_layer = 45
|
||
support_material_interface_fan_speed = -1
|
||
temperature_vitrification = 45
|
||
textured_cool_plate_temp = 40
|
||
textured_cool_plate_temp_initial_layer = 40
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
|
||
[filament:Elas PLA Pro @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFA00
|
||
instantiation = false
|
||
activate_air_filtration = 0
|
||
activate_chamber_temp_control = 0
|
||
adaptive_pressure_advance = 0
|
||
adaptive_pressure_advance_bridges = 0
|
||
adaptive_pressure_advance_model = 0,0,0
|
||
0,0,0
|
||
adaptive_pressure_advance_overhangs = 0
|
||
additional_cooling_fan_speed = 70
|
||
chamber_temperature = 0
|
||
close_fan_the_first_x_layers = 1
|
||
complete_print_exhaust_fan_speed = 70
|
||
cool_plate_temp = 35
|
||
cool_plate_temp_initial_layer = 35
|
||
default_filament_colour =
|
||
dont_slow_down_outer_wall = 0
|
||
during_print_exhaust_fan_speed = 70
|
||
enable_overhang_bridge_fan = 1
|
||
enable_pressure_advance = 1
|
||
eng_plate_temp = 60
|
||
eng_plate_temp_initial_layer = 60
|
||
fan_cooling_layer_time = 100
|
||
fan_max_speed = 100
|
||
fan_min_speed = 100
|
||
filament_cooling_final_speed = 0
|
||
filament_cooling_initial_speed = 0
|
||
filament_cooling_moves = 0
|
||
filament_cost = 500
|
||
filament_density = 1.24
|
||
filament_deretraction_speed = nil
|
||
filament_diameter = 1.75
|
||
filament_flow_ratio = 1.025
|
||
filament_is_support = 0
|
||
filament_loading_speed = 0
|
||
filament_loading_speed_start = 0
|
||
filament_long_retractions_when_cut = nil
|
||
filament_max_volumetric_speed = 18
|
||
filament_minimal_purge_on_wipe_tower = 0
|
||
filament_multitool_ramming = 0
|
||
filament_multitool_ramming_flow = 10
|
||
filament_multitool_ramming_volume = 10
|
||
filament_notes =
|
||
filament_retract_before_wipe = nil
|
||
filament_retract_lift_above = nil
|
||
filament_retract_lift_below = nil
|
||
filament_retract_lift_enforce = nil
|
||
filament_retract_restart_extra = nil
|
||
filament_retract_when_changing_layer = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
filament_retraction_length = nil
|
||
filament_retraction_minimum_travel = nil
|
||
filament_retraction_speed = nil
|
||
filament_shrink = 100%
|
||
filament_shrinkage_compensation_z = 100%
|
||
filament_soluble = 0
|
||
filament_stamping_distance = 0
|
||
filament_stamping_loading_speed = 0
|
||
filament_toolchange_delay = 0
|
||
filament_unloading_speed = 0
|
||
filament_unloading_speed_start = 0
|
||
filament_vendor = Elas
|
||
filament_wipe = nil
|
||
filament_wipe_distance = nil
|
||
filament_z_hop = nil
|
||
filament_z_hop_types = nil
|
||
full_fan_speed_layer = 0
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
idle_temperature = 0
|
||
internal_bridge_fan_speed = -1
|
||
ironing_fan_speed = -1
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
overhang_fan_speed = 100
|
||
overhang_fan_threshold = 50%
|
||
pellet_flow_coefficient = 0.4157
|
||
pressure_advance = 0.06
|
||
reduce_fan_stop_start_freq = 1
|
||
required_nozzle_HRC = 3
|
||
slow_down_for_layer_cooling = 1
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 10
|
||
supertack_plate_temp = 45
|
||
supertack_plate_temp_initial_layer = 45
|
||
support_material_interface_fan_speed = -1
|
||
temperature_vitrification = 45
|
||
textured_cool_plate_temp = 40
|
||
textured_cool_plate_temp_initial_layer = 40
|
||
textured_plate_temp = 60
|
||
textured_plate_temp_initial_layer = 60
|
||
|
||
[filament:Elegoo PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFE04
|
||
instantiation = false
|
||
filament_cost = 0
|
||
filament_density = 1.25
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Elegoo
|
||
filament_start_gcode = ; filament start gcode
|
||
|
||
[filament:Elegoo PLA Matte @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = EPLAMB00
|
||
instantiation = false
|
||
filament_cost = 0
|
||
filament_density = 1.25
|
||
filament_vendor = Elegoo
|
||
filament_start_gcode = ; filament start gcode
|
||
|
||
[filament:Elegoo PLA Silk @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = EPLASB00
|
||
instantiation = false
|
||
filament_cost = 0
|
||
filament_density = 1.32
|
||
filament_vendor = Elegoo
|
||
filament_max_volumetric_speed = 16
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
filament_start_gcode = ; filament start gcode
|
||
|
||
[filament:Elegoo PLA-CF @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = EPLACFB00
|
||
instantiation = false
|
||
additional_cooling_fan_speed = 0
|
||
cool_plate_temp = 45
|
||
cool_plate_temp_initial_layer = 45
|
||
filament_type = PLA-CF
|
||
filament_vendor = Elegoo
|
||
filament_density = 1.21
|
||
required_nozzle_HRC = 40
|
||
slow_down_layer_time = 7
|
||
filament_start_gcode = ; Filament start gcode
|
||
|
||
filament_end_gcode = ; filament end gcode
|
||
|
||
[filament:Elegoo Rapid PLA+ @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFE05
|
||
instantiation = false
|
||
filament_max_volumetric_speed = 21
|
||
filament_density = 1.25
|
||
filament_vendor = Elegoo
|
||
filament_start_gcode = ; filament start gcode
|
||
|
||
[filament:Eolas Prints PLA Antibacterial @System]
|
||
filament_id = GFSEP008
|
||
setting_id = GFSEP008_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 216
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_low = 195
|
||
nozzle_temperature_range_high = 230
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.24
|
||
filament_cost = 30.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:Eolas Prints PLA High Speed @System]
|
||
filament_id = GFSEP005
|
||
setting_id = GFSEP005_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_low = 210
|
||
nozzle_temperature_range_high = 240
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.24
|
||
filament_cost = 25.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 17.8
|
||
|
||
[filament:Eolas Prints PLA INGEO 850 @System]
|
||
filament_id = GFSEP006
|
||
setting_id = GFSEP006_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 210
|
||
nozzle_temperature_initial_layer = 215
|
||
nozzle_temperature_range_low = 190
|
||
nozzle_temperature_range_high = 230
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.24
|
||
filament_cost = 25.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:Eolas Prints PLA INGEO 870 @System]
|
||
filament_id = GFSEP007
|
||
setting_id = GFSEP007_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 225
|
||
nozzle_temperature_range_low = 200
|
||
nozzle_temperature_range_high = 235
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.22
|
||
filament_cost = 30.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:Eolas Prints PLA Matte @System]
|
||
filament_id = GFSEP002
|
||
setting_id = GFSEP002_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 215
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_low = 200
|
||
nozzle_temperature_range_high = 230
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.24
|
||
filament_cost = 25.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:Eolas Prints PLA Neon @System]
|
||
filament_id = GFSEP004
|
||
setting_id = GFSEP004_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 210
|
||
nozzle_temperature_initial_layer = 215
|
||
nozzle_temperature_range_low = 200
|
||
nozzle_temperature_range_high = 230
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.24
|
||
filament_cost = 25.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 10
|
||
|
||
[filament:Eolas Prints PLA Premium @System]
|
||
filament_id = GFSEP001
|
||
setting_id = GFSEP001_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 210
|
||
nozzle_temperature_initial_layer = 215
|
||
nozzle_temperature_range_low = 190
|
||
nozzle_temperature_range_high = 230
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.24
|
||
filament_cost = 19.90
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:Eolas Prints PLA Silk @System]
|
||
filament_id = GFSEP003
|
||
setting_id = GFSEP003_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 215
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_low = 205
|
||
nozzle_temperature_range_high = 235
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.24
|
||
filament_cost = 25.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 8
|
||
|
||
[filament:Eolas Prints PLA Transition @System]
|
||
filament_id = GFSEP009
|
||
setting_id = GFSEP009_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_pla
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = PLA
|
||
nozzle_temperature = 210
|
||
nozzle_temperature_initial_layer = 215
|
||
nozzle_temperature_range_low = 200
|
||
nozzle_temperature_range_high = 230
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.24
|
||
filament_cost = 13.90
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 15
|
||
|
||
[filament:FDplast PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = FDPLAST04
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 16
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = FDplast
|
||
nozzle_temperature = 215
|
||
nozzle_temperature_initial_layer = 215
|
||
nozzle_temperature_range_high = 225
|
||
nozzle_temperature_range_low = 190
|
||
hot_plate_temp = 65
|
||
hot_plate_temp_initial_layer = 65
|
||
textured_plate_temp = 65
|
||
textured_plate_temp_initial_layer = 65
|
||
|
||
[filament:FILL3D PLA Turbo @base]
|
||
from = system
|
||
filament_id = FILL3D001
|
||
instantiation = false
|
||
inherits = fdm_filament_pla
|
||
adaptive_pressure_advance = 1
|
||
adaptive_pressure_advance_model = 0.03,23.43,5000
|
||
0.028,25.31,5000
|
||
0.025,28.12,5000
|
||
0.025,23.43,12000
|
||
0.020,25.31,12000
|
||
0.018,28.12,12000
|
||
additional_cooling_fan_speed = 70
|
||
cool_plate_temp = 35
|
||
cool_plate_temp_initial_layer = 35
|
||
enable_pressure_advance = 1
|
||
fan_cooling_layer_time = 100
|
||
fan_max_speed = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 25.4
|
||
filament_density = 1.31
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 32
|
||
filament_type = PLA
|
||
filament_vendor = FILL3D
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 55
|
||
nozzle_temperature = 235
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
pressure_advance = 0.036
|
||
slow_down_layer_time = 4
|
||
slow_down_min_speed = 10
|
||
supertack_plate_temp = 45
|
||
supertack_plate_temp_initial_layer = 45
|
||
temperature_vitrification = 45
|
||
textured_plate_temp = 55
|
||
textured_plate_temp_initial_layer = 55
|
||
|
||
[filament:Generic PLA @System]
|
||
renamed_from = My Generic PLA
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
setting_id = OGFSA04
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Generic PLA High Speed @System]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
setting_id = OGFSL95_00
|
||
filament_id = OGFL95
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 18
|
||
slow_down_layer_time = 4
|
||
compatible_printers =
|
||
|
||
[filament:Generic PLA Matte @System]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
setting_id = OGFSL99_02
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 11
|
||
filament_retraction_length = 0.8
|
||
compatible_printers =
|
||
|
||
[filament:Generic PLA-CF @System]
|
||
renamed_from = My Generic PLA-CF
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFL98
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_type = PLA-CF
|
||
compatible_printers =
|
||
|
||
[filament:NIT PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = NIT02
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 12
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = NIT
|
||
nozzle_temperature = 210
|
||
nozzle_temperature_initial_layer = 210
|
||
nozzle_temperature_range_high = 210
|
||
nozzle_temperature_range_low = 200
|
||
|
||
[filament:Numakers PLA+ @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFNMK00
|
||
instantiation = false
|
||
filament_cost = 20.99
|
||
filament_density = 1.24
|
||
filament_flow_ratio = 0.99
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Numakers
|
||
nozzle_temperature = 225
|
||
nozzle_temperature_initial_layer = 225
|
||
nozzle_temperature_range_high = 255
|
||
nozzle_temperature_range_low = 200
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_height = 10%
|
||
filament_scarf_gap = 0%
|
||
filament_scarf_length = 10
|
||
temperature_vitrification = 55
|
||
|
||
[filament:Overture Air PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = GFOT006
|
||
instantiation = false
|
||
filament_cost = 27.99
|
||
filament_density = 0.82
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 8
|
||
filament_vendor = Overture
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 220
|
||
nozzle_temperature_range_low = 190
|
||
slow_down_layer_time = 4
|
||
temperature_vitrification = 64
|
||
|
||
[filament:Overture Easy PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = GFOT003
|
||
instantiation = false
|
||
filament_cost = 17.99
|
||
filament_density = 1.2
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Overture
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 220
|
||
nozzle_temperature_range_low = 190
|
||
slow_down_layer_time = 4
|
||
temperature_vitrification = 66
|
||
|
||
[filament:Overture Matte PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL05
|
||
instantiation = false
|
||
filament_cost = 24.52
|
||
filament_density = 1.22
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Overture
|
||
slow_down_layer_time = 6
|
||
|
||
[filament:Overture PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL04
|
||
instantiation = false
|
||
filament_cost = 24.15
|
||
filament_density = 1.2
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Overture
|
||
slow_down_layer_time = 6
|
||
|
||
[filament:Overture PLA Pro @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = GFOT001
|
||
instantiation = false
|
||
filament_cost = 26.99
|
||
filament_density = 1.27
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Overture
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 220
|
||
nozzle_temperature_range_low = 190
|
||
slow_down_layer_time = 4
|
||
temperature_vitrification = 64
|
||
|
||
[filament:Overture Rock PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = GFOT004
|
||
instantiation = false
|
||
filament_cost = 24.99
|
||
filament_density = 1.3
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 20
|
||
filament_vendor = Overture
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 230
|
||
nozzle_temperature_range_low = 190
|
||
slow_down_layer_time = 4
|
||
temperature_vitrification = 63
|
||
|
||
[filament:Overture Silk PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = GFOT002
|
||
instantiation = false
|
||
filament_cost = 25.99
|
||
filament_density = 1.19
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Overture
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 220
|
||
nozzle_temperature_range_low = 200
|
||
slow_down_layer_time = 4
|
||
temperature_vitrification = 58
|
||
|
||
[filament:Overture Super PLA+ @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = GFOT005
|
||
instantiation = false
|
||
filament_cost = 28.99
|
||
filament_density = 1.21
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Overture
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 230
|
||
nozzle_temperature_range_low = 190
|
||
slow_down_layer_time = 4
|
||
temperature_vitrification = 63
|
||
|
||
[filament:Panchroma CoPE @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM016
|
||
instantiation = false
|
||
filament_cost = 19.99
|
||
filament_density = 1.29
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 58
|
||
|
||
[filament:Panchroma PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM001
|
||
instantiation = false
|
||
filament_cost = 19.99
|
||
filament_density = 1.32
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 58
|
||
|
||
[filament:Panchroma PLA Celestial @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM008
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Galaxy @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM007
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Glow @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM010
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Luminous @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM011
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Marble @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM003
|
||
instantiation = false
|
||
filament_cost = 21.99
|
||
filament_density = 1.31
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Matte @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM002
|
||
instantiation = false
|
||
filament_cost = 20.99
|
||
filament_density = 1.31
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Metallic @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM012
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Neon @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM013
|
||
instantiation = false
|
||
filament_cost = 24.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Satin @base]
|
||
renamed_from = Panchroma PLA Stain @base
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM005
|
||
instantiation = false
|
||
filament_cost = 20.99
|
||
filament_density = 1.24
|
||
filament_flow_ratio = 0.95
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 59
|
||
|
||
[filament:Panchroma PLA Silk @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM004
|
||
instantiation = false
|
||
filament_cost = 24.99
|
||
filament_density = 1.31
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 58
|
||
|
||
[filament:Panchroma PLA Starlight @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM009
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Temp Shift @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM015
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA Translucent @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM006
|
||
instantiation = false
|
||
filament_cost = 24.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:Panchroma PLA UV Shift @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM014
|
||
instantiation = false
|
||
filament_cost = 29.99
|
||
filament_density = 1.17
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 61
|
||
|
||
[filament:PolyLite PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL00
|
||
instantiation = false
|
||
filament_cost = 25.4
|
||
filament_flow_ratio = 0.95
|
||
filament_vendor = Polymaker
|
||
|
||
[filament:PolyLite PLA Pro @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM019
|
||
instantiation = false
|
||
filament_cost = 24.99
|
||
filament_density = 1.22
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 220
|
||
nozzle_temperature_range_low = 190
|
||
temperature_vitrification = 62
|
||
|
||
[filament:PolyTerra PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL01
|
||
instantiation = false
|
||
filament_cost = 25.4
|
||
filament_density = 1.31
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = Polymaker
|
||
|
||
[filament:Polymaker HT-PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM017
|
||
instantiation = false
|
||
filament_cost = 26.99
|
||
filament_density = 1.28
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
hot_plate_temp = 65
|
||
hot_plate_temp_initial_layer = 65
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 230
|
||
nozzle_temperature_range_low = 210
|
||
temperature_vitrification = 60
|
||
textured_plate_temp = 65
|
||
textured_plate_temp_initial_layer = 65
|
||
|
||
[filament:Polymaker HT-PLA-GF @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFPM018
|
||
instantiation = false
|
||
filament_cost = 32.99
|
||
filament_density = 1.34
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = Polymaker
|
||
hot_plate_temp = 65
|
||
hot_plate_temp_initial_layer = 65
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 230
|
||
nozzle_temperature_range_low = 210
|
||
temperature_vitrification = 60
|
||
textured_plate_temp = 65
|
||
textured_plate_temp_initial_layer = 65
|
||
|
||
[filament:SUNLU PLA Marble @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFSNL06
|
||
instantiation = false
|
||
filament_cost = 31.99
|
||
filament_density = 1.25
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = SUNLU
|
||
|
||
[filament:SUNLU PLA Matte @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFSNL02
|
||
instantiation = false
|
||
filament_cost = 25.99
|
||
filament_density = 1.3
|
||
filament_flow_ratio = 0.98
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = SUNLU
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_height = 5%
|
||
filament_scarf_gap = 0%
|
||
filament_scarf_length = 10
|
||
temperature_vitrification = 54
|
||
nozzle_temperature_range_high = 245
|
||
nozzle_temperature_range_low = 205
|
||
|
||
[filament:SUNLU PLA+ 2.0 @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFSNL04
|
||
instantiation = false
|
||
filament_cost = 18.99
|
||
filament_density = 1.21
|
||
filament_flow_ratio = 1.0
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = SUNLU
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_height = 5%
|
||
filament_scarf_gap = 0%
|
||
filament_scarf_length = 10
|
||
temperature_vitrification = 54
|
||
|
||
[filament:SUNLU PLA+ @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFSNL03
|
||
instantiation = false
|
||
filament_cost = 18.99
|
||
filament_density = 1.23
|
||
filament_flow_ratio = 1.0
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = SUNLU
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_height = 5%
|
||
filament_scarf_gap = 0%
|
||
filament_scarf_length = 10
|
||
temperature_vitrification = 54
|
||
|
||
[filament:SUNLU Silk PLA+ @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFSNL05
|
||
instantiation = false
|
||
description = To make the prints get higher gloss, please dry the filament before use, and set the outer wall speed to be 40 to 60 mm/s when slicing.
|
||
filament_cost = 29.99
|
||
filament_density = 1.25
|
||
filament_flow_ratio = 0.98
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = SUNLU
|
||
filament_scarf_height = 5%
|
||
filament_scarf_gap = 0%
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
supertack_plate_temp = 0
|
||
supertack_plate_temp_initial_layer = 0
|
||
temperature_vitrification = 54
|
||
|
||
[filament:SUNLU Wood PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFSNL07
|
||
instantiation = false
|
||
filament_cost = 26.99
|
||
filament_density = 1.10
|
||
filament_flow_ratio = 1.0
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_retraction_length = 4
|
||
filament_retraction_speed = 50
|
||
filament_deretraction_speed = 0
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = SUNLU
|
||
filament_scarf_seam_type = none
|
||
filament_scarf_height = 5%
|
||
filament_scarf_gap = 0%
|
||
filament_scarf_length = 10
|
||
temperature_vitrification = 54
|
||
|
||
[filament:Valment PLA @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = VLMNT01
|
||
instantiation = false
|
||
filament_cost = 670
|
||
filament_type = PLA
|
||
default_filament_colour = #124943
|
||
filament_density = 1.24
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Valment
|
||
slow_down_layer_time = 6
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 225
|
||
nozzle_temperature_range_low = 200
|
||
nozzle_temperature_range_high = 250
|
||
filament_notes = Bu filament ayarları GlauTech tarafından oluşturulmuştur. Filamentin daha verimli çalışması için, slicerdaki kalibrasyon ayarlarının tek tek yapılması önemlidir. Kalibrasyon ayarları için, GlauTech youtube kanalından destek alabilirsiniz.
|
||
|
||
Boş Makara Ağırlığı: 150gr
|
||
slow_down_min_speed = 20
|
||
complete_print_exhaust_fan_speed = 80
|
||
during_print_exhaust_fan_speed = 60
|
||
additional_cooling_fan_speed = 100
|
||
|
||
[filament:Valment PLA Galaxy @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = VLMNT04
|
||
instantiation = false
|
||
filament_cost = 850
|
||
filament_type = PLA
|
||
default_filament_colour = #124943
|
||
filament_density = 1.24
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Valment
|
||
slow_down_layer_time = 6
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 245
|
||
nozzle_temperature_range_low = 220
|
||
nozzle_temperature_range_high = 250
|
||
filament_notes = Bu filament ayarları GlauTech tarafından oluşturulmuştur. Filamentin daha verimli çalışması için, slicerdaki kalibrasyon ayarlarının tek tek yapılması önemlidir. Kalibrasyon ayarları için, GlauTech youtube kanalından destek alabilirsiniz.
|
||
|
||
Galaxy filamentlerimizde;
|
||
0.2mm nozul kullanılmaması,
|
||
0.16mm katman yüksekliği altına inilmemesi önerilir.
|
||
|
||
Boş Makara Ağırlığı: 150gr
|
||
slow_down_min_speed = 20
|
||
complete_print_exhaust_fan_speed = 80
|
||
during_print_exhaust_fan_speed = 60
|
||
additional_cooling_fan_speed = 100
|
||
|
||
[filament:Valment PLA Silk @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = VLMNT02
|
||
instantiation = false
|
||
filament_cost = 710
|
||
filament_type = PLA
|
||
filament_density = 1.24
|
||
default_filament_colour = #124943
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 7.5
|
||
filament_vendor = Valment
|
||
slow_down_layer_time = 6
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 245
|
||
nozzle_temperature_range_low = 220
|
||
nozzle_temperature_range_high = 250
|
||
filament_notes = Bu filament ayarları GlauTech tarafından oluşturulmuştur. Filamentin daha verimli çalışması için, slicerdaki kalibrasyon ayarlarının tek tek yapılması önemlidir. Kalibrasyon ayarları için, GlauTech youtube kanalından destek alabilirsiniz.
|
||
|
||
Boş Makara Ağırlığı: 150gr
|
||
slow_down_min_speed = 20
|
||
complete_print_exhaust_fan_speed = 80
|
||
during_print_exhaust_fan_speed = 60
|
||
additional_cooling_fan_speed = 100
|
||
|
||
[filament:Valment PLA-CF @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = VLMNT03
|
||
instantiation = false
|
||
filament_cost = 1400
|
||
filament_type = PLA-CF
|
||
default_filament_colour = #124943
|
||
filament_density = 1.24
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = Valment
|
||
slow_down_layer_time = 6
|
||
nozzle_temperature = 225
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_low = 200
|
||
nozzle_temperature_range_high = 250
|
||
filament_notes = Bu filament ayarları GlauTech tarafından oluşturulmuştur. Filamentin daha verimli çalışması için, slicerdaki kalibrasyon ayarlarının tek tek yapılması önemlidir. Kalibrasyon ayarları için, GlauTech youtube kanalından destek alabilirsiniz.
|
||
|
||
Boş Makara Ağırlığı: 150gr
|
||
slow_down_min_speed = 20
|
||
complete_print_exhaust_fan_speed = 80
|
||
during_print_exhaust_fan_speed = 60
|
||
additional_cooling_fan_speed = 100
|
||
|
||
[filament:eSUN PLA+ @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL03
|
||
instantiation = false
|
||
filament_cost = 22.99
|
||
filament_density = 1.25
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 12
|
||
filament_vendor = eSUN
|
||
slow_down_layer_time = 6
|
||
|
||
[filament:eSUN PLA-Basic @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL04
|
||
instantiation = false
|
||
filament_cost = 11.99
|
||
filament_density = 1.24
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
filament_vendor = eSUN
|
||
slow_down_layer_time = 6
|
||
|
||
[filament:eSUN PLA-Marble @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL06
|
||
instantiation = false
|
||
filament_cost = 28.99
|
||
filament_density = 1.27
|
||
filament_flow_ratio = 0.99
|
||
filament_max_volumetric_speed = 8
|
||
filament_vendor = eSUN
|
||
slow_down_layer_time = 6
|
||
|
||
[filament:eSUN PLA-Matte @base]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL05
|
||
instantiation = false
|
||
filament_cost = 14.99
|
||
filament_density = 1.32
|
||
filament_flow_ratio = 0.99
|
||
filament_max_volumetric_speed = 8
|
||
filament_vendor = eSUN
|
||
slow_down_layer_time = 6
|
||
|
||
[filament:eSUN ePLA-LW @System]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
setting_id = LWSL02_00
|
||
filament_id = ESN02
|
||
instantiation = true
|
||
filament_type = PLA-AERO
|
||
filament_cost = 33.99
|
||
filament_density = 1.2
|
||
filament_flow_ratio = 0.48
|
||
filament_max_volumetric_speed = 6
|
||
filament_vendor = eSUN
|
||
filament_scarf_seam_type = none
|
||
nozzle_temperature = 243
|
||
nozzle_temperature_initial_layer = 243
|
||
nozzle_temperature_range_low = 190
|
||
nozzle_temperature_range_high = 270
|
||
temperature_vitrification = 53
|
||
compatible_printers =
|
||
|
||
[filament:fdm_filament_pla_silk]
|
||
inherits = fdm_filament_pla
|
||
from = system
|
||
filament_id = OGFL96
|
||
instantiation = false
|
||
description = To make the prints get higher gloss, please dry the filament before use, and set the outer wall speed to be 40 to 60 mm/s when slicing.
|
||
filament_flow_ratio = 0.98
|
||
slow_down_layer_time = 8
|
||
|
||
[filament:Generic PP @System]
|
||
inherits = fdm_filament_pp
|
||
from = system
|
||
setting_id = OGFSP97_00
|
||
instantiation = true
|
||
description = This is neither a commonly used filament, nor one of Bambu filaments, and it varies a lot from brand to brand. So, it's highly recommended to ask its vendor for suitable profile before printing and adjust some parameters according to its performances.
|
||
compatible_printers =
|
||
|
||
[filament:Generic PP-CF @System]
|
||
inherits = fdm_filament_pp
|
||
from = system
|
||
setting_id = OGFSP96_00
|
||
instantiation = true
|
||
description = This is neither a commonly used filament, nor one of Bambu filaments, and it varies a lot from brand to brand. So, it's highly recommended to ask its vendor for suitable profile before printing and adjust some parameters according to its performances.
|
||
filament_cost = 77.99
|
||
filament_density = 1.01
|
||
filament_max_volumetric_speed = 6
|
||
filament_type = PP-CF
|
||
compatible_printers =
|
||
|
||
[filament:Generic PP-GF @System]
|
||
inherits = fdm_filament_pp
|
||
from = system
|
||
setting_id = OGFSP97_03
|
||
instantiation = true
|
||
description = This is neither a commonly used filament, nor one of Bambu filaments, and it varies a lot from brand to brand. So, it's highly recommended to ask its vendor for suitable profile before printing and adjust some parameters according to its performances.
|
||
filament_cost = 59.99
|
||
filament_density = 1.05
|
||
filament_max_volumetric_speed = 6
|
||
filament_type = PP-GF
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PPA-CF @base]
|
||
inherits = fdm_filament_ppa
|
||
from = system
|
||
filament_id = OGFN06
|
||
instantiation = false
|
||
filament_vendor = Bambu Lab
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
|
||
[filament:Generic PPA-CF @System]
|
||
inherits = fdm_filament_ppa
|
||
from = system
|
||
setting_id = OGFSN97_00
|
||
instantiation = true
|
||
fan_max_speed = 35
|
||
filament_max_volumetric_speed = 6.5
|
||
overhang_fan_threshold = 25%
|
||
filament_type = PPA-CF
|
||
compatible_printers =
|
||
|
||
[filament:Generic PPA-GF @System]
|
||
inherits = fdm_filament_ppa
|
||
from = system
|
||
setting_id = OGFSN96_00
|
||
filament_id = OGFN96
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 6
|
||
filament_type = PPA-GF
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PPS-CF @base]
|
||
inherits = fdm_filament_pps
|
||
from = system
|
||
filament_id = OGFT02
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of nozzle clogging, oozing, warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
fan_max_speed = 30
|
||
filament_cost = 175
|
||
filament_density = 1.26
|
||
filament_max_volumetric_speed = 6
|
||
filament_type = PPS-CF
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature_range_low = 310
|
||
overhang_fan_threshold = 25%
|
||
required_nozzle_HRC = 40
|
||
temperature_vitrification = 220
|
||
|
||
[filament:Bambu PVA @base]
|
||
inherits = fdm_filament_pva
|
||
from = system
|
||
filament_id = OGFS04
|
||
instantiation = false
|
||
description = This is a water-soluble support filament, and usually it is only for the support structure and not for the model body. Printing this filament is of many requirements, and to get better printing quality, please refer to this wiki: PVA Printing Guide.
|
||
filament_cost = 79.98
|
||
filament_density = 1.27
|
||
filament_max_volumetric_speed = 6
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature_range_high = 250
|
||
nozzle_temperature_range_low = 210
|
||
slow_down_layer_time = 7
|
||
slow_down_min_speed = 20
|
||
|
||
[filament:Generic PVA @System]
|
||
renamed_from = My Generic PVA
|
||
inherits = fdm_filament_pva
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFS99
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:FDplast SBS @base]
|
||
inherits = fdm_filament_sbs
|
||
from = system
|
||
filament_id = FDPLAST05
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 27
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = FDplast
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_high = 240
|
||
nozzle_temperature_range_low = 225
|
||
hot_plate_temp = 80
|
||
hot_plate_temp_initial_layer = 80
|
||
textured_plate_temp = 80
|
||
textured_plate_temp_initial_layer = 80
|
||
|
||
[filament:Generic SBS @System]
|
||
inherits = fdm_filament_sbs
|
||
from = system
|
||
setting_id = OGFSL99
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu TPU 95A @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = OGFU01
|
||
instantiation = false
|
||
description = This filament is too soft and not compatible with the AMS. Printing it is of many requirements, and to get better printing quality, please refer to this wiki: TPU printing guide.
|
||
filament_cost = 41.99
|
||
filament_density = 1.22
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
|
||
[filament:Bambu TPU 95A HF @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = OGFU00
|
||
instantiation = false
|
||
description = This filament is too soft and not compatible with the AMS. Printing it is of many requirements, and to get better printing quality, please refer to this wiki: TPU printing guide.
|
||
filament_cost = 41.99
|
||
filament_density = 1.22
|
||
filament_max_volumetric_speed = 12
|
||
filament_retraction_length = 0.8
|
||
filament_vendor = Bambu Lab
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
|
||
[filament:COEX TPE 30D @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = CX30DB20
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 80.00
|
||
filament_density = 1.15
|
||
filament_type = TPU
|
||
filament_notes = Flexible filament - print slowly with minimal retraction
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 240
|
||
bed_temperature = 30
|
||
bed_temperature_initial_layer = 35
|
||
temperature_vitrification = 60
|
||
filament_max_volumetric_speed = 3.5
|
||
filament_retraction_minimum_travel = 3
|
||
filament_retract_before_wipe = 0%
|
||
filament_retract_layer_change = 0
|
||
filament_retract_when_changing_layer = 0
|
||
filament_retraction_length = 0.4
|
||
filament_retraction_speed = 20
|
||
filament_deretraction_speed = 20
|
||
filament_wipe = 0
|
||
filament_wipe_distance = 0
|
||
fan_min_speed = 80
|
||
fan_max_speed = 100
|
||
disable_fan_first_layers = 1
|
||
full_fan_speed_layer = 2
|
||
slow_down_layer_time = 10
|
||
slow_down_min_speed = 5
|
||
enable_pressure_advance = 0
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:COEX TPE 40D @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = CX40DB20
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 80.00
|
||
filament_density = 1.18
|
||
filament_type = TPU
|
||
filament_notes = Flexible filament - print slowly with minimal retraction
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 240
|
||
bed_temperature = 30
|
||
bed_temperature_initial_layer = 35
|
||
temperature_vitrification = 60
|
||
filament_max_volumetric_speed = 5.5
|
||
filament_retraction_minimum_travel = 3
|
||
filament_retract_before_wipe = 0%
|
||
filament_retract_layer_change = 0
|
||
filament_retract_when_changing_layer = 0
|
||
filament_retraction_length = 0.4
|
||
filament_retraction_speed = 20
|
||
filament_deretraction_speed = 20
|
||
filament_wipe = 0
|
||
filament_wipe_distance = 0
|
||
fan_min_speed = 80
|
||
fan_max_speed = 100
|
||
disable_fan_first_layers = 1
|
||
full_fan_speed_layer = 2
|
||
slow_down_layer_time = 10
|
||
slow_down_min_speed = 5
|
||
enable_pressure_advance = 0
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:COEX TPE 60D @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = CX60DB19
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 80.00
|
||
filament_density = 1.20
|
||
filament_type = TPU
|
||
filament_notes = Flexible filament - print slowly with minimal retraction
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 240
|
||
bed_temperature = 30
|
||
bed_temperature_initial_layer = 35
|
||
temperature_vitrification = 60
|
||
filament_max_volumetric_speed = 6.5
|
||
filament_retraction_minimum_travel = 3
|
||
filament_retract_before_wipe = 0%
|
||
filament_retract_layer_change = 0
|
||
filament_retract_when_changing_layer = 0
|
||
filament_retraction_length = 0.4
|
||
filament_retraction_speed = 20
|
||
filament_deretraction_speed = 20
|
||
filament_wipe = 0
|
||
filament_wipe_distance = 0
|
||
fan_min_speed = 80
|
||
fan_max_speed = 100
|
||
disable_fan_first_layers = 1
|
||
full_fan_speed_layer = 2
|
||
slow_down_layer_time = 10
|
||
slow_down_min_speed = 5
|
||
enable_pressure_advance = 0
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:COEX TPU 60A @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = CX60AB17
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 95.00
|
||
filament_density = 1.14
|
||
filament_type = TPU
|
||
filament_notes = Flexible filament - print slowly with minimal retraction
|
||
nozzle_temperature = 225
|
||
nozzle_temperature_initial_layer = 225
|
||
bed_temperature = 0
|
||
bed_temperature_initial_layer = 0
|
||
temperature_vitrification = 60
|
||
filament_max_volumetric_speed = 1
|
||
filament_retraction_minimum_travel = 3
|
||
filament_retract_before_wipe = 0%
|
||
filament_retract_layer_change = 0
|
||
filament_retract_when_changing_layer = 0
|
||
filament_retraction_length = 0
|
||
filament_retraction_speed = 20
|
||
filament_deretraction_speed = 20
|
||
filament_wipe = 0
|
||
filament_wipe_distance = 0
|
||
fan_min_speed = 80
|
||
fan_max_speed = 100
|
||
disable_fan_first_layers = 1
|
||
full_fan_speed_layer = 2
|
||
slow_down_layer_time = 10
|
||
slow_down_min_speed = 5
|
||
enable_pressure_advance = 0
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:Elegoo TPU 95A @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = OGFE07
|
||
instantiation = false
|
||
filament_max_volumetric_speed = 3.6
|
||
filament_vendor = Elegoo
|
||
filament_density = 1.21
|
||
nozzle_temperature = 225
|
||
nozzle_temperature_initial_layer = 225
|
||
filament_start_gcode = ; filament start gcode
|
||
|
||
[filament:Elegoo TPU @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = ETPUB00
|
||
instantiation = false
|
||
filament_max_volumetric_speed = 3.6
|
||
filament_vendor = Elegoo
|
||
filament_density = 1.21
|
||
nozzle_temperature = 225
|
||
nozzle_temperature_initial_layer = 225
|
||
filament_start_gcode = ; filament start gcode
|
||
|
||
[filament:Eolas Prints TPU D60 UV Resistant @System]
|
||
filament_id = GFSEP015
|
||
setting_id = GFSEP015_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_tpu
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = TPU
|
||
nozzle_temperature = 225
|
||
nozzle_temperature_initial_layer = 230
|
||
nozzle_temperature_range_low = 215
|
||
nozzle_temperature_range_high = 245
|
||
hot_plate_temp = 55
|
||
hot_plate_temp_initial_layer = 60
|
||
filament_density = 1.16
|
||
filament_cost = 37.90
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 8
|
||
|
||
[filament:Eolas Prints TPU Flex 93A @System]
|
||
filament_id = GFSEP013
|
||
setting_id = GFSEP013_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_tpu
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = TPU
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 225
|
||
nozzle_temperature_range_low = 210
|
||
nozzle_temperature_range_high = 240
|
||
hot_plate_temp = 50
|
||
hot_plate_temp_initial_layer = 55
|
||
filament_density = 1.21
|
||
filament_cost = 34.99
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 6
|
||
|
||
[filament:Eolas Prints TPU Flex D53 @System]
|
||
filament_id = GFSEP014
|
||
setting_id = GFSEP014_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_tpu
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = TPU
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 225
|
||
nozzle_temperature_range_low = 205
|
||
nozzle_temperature_range_high = 235
|
||
hot_plate_temp = 45
|
||
hot_plate_temp_initial_layer = 50
|
||
filament_density = 1.17
|
||
filament_cost = 38.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 8
|
||
|
||
[filament:Eolas Prints TPU Transition @System]
|
||
filament_id = GFSEP016
|
||
setting_id = GFSEP016_00
|
||
from = system
|
||
instantiation = true
|
||
inherits = fdm_filament_tpu
|
||
filament_color = #4d9398
|
||
filament_vendor = Eolas Prints
|
||
filament_type = TPU
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 225
|
||
nozzle_temperature_range_low = 210
|
||
nozzle_temperature_range_high = 240
|
||
hot_plate_temp = 50
|
||
hot_plate_temp_initial_layer = 55
|
||
filament_density = 1.21
|
||
filament_cost = 22.50
|
||
filament_spool_weight = 1000
|
||
filament_max_volumetric_speed = 5
|
||
|
||
[filament:FDplast TPU @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = FDPLAST06
|
||
instantiation = false
|
||
description = When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.
|
||
filament_cost = 27
|
||
filament_density = 1.26
|
||
filament_flow_ratio = 0.98
|
||
filament_vendor = FDplast
|
||
nozzle_temperature = 180
|
||
nozzle_temperature_initial_layer = 180
|
||
nozzle_temperature_range_high = 190
|
||
nozzle_temperature_range_low = 175
|
||
hot_plate_temp = 60
|
||
hot_plate_temp_initial_layer = 60
|
||
textured_plate_temp = 60
|
||
textured_plate_temp_initial_layer = 60
|
||
|
||
[filament:Generic TPU @System]
|
||
renamed_from = My Generic TPU
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
setting_id = OGFSA04
|
||
filament_id = OGFU99
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Overture TPU @base]
|
||
inherits = fdm_filament_tpu
|
||
from = system
|
||
filament_id = GFOT008
|
||
instantiation = false
|
||
fan_cooling_layer_time = 100
|
||
fan_max_speed = 100
|
||
fan_min_speed = 100
|
||
filament_cost = 29.99
|
||
filament_density = 1.18
|
||
filament_flow_ratio = 1
|
||
filament_max_volumetric_speed = 10
|
||
filament_vendor = Overture
|
||
nozzle_temperature = 220
|
||
nozzle_temperature_initial_layer = 220
|
||
nozzle_temperature_range_high = 230
|
||
nozzle_temperature_range_low = 210
|
||
slow_down_layer_time = 15
|
||
temperature_vitrification = 30
|
||
|
||
[filament:Bambu ABS @System]
|
||
inherits = Bambu ABS @base
|
||
from = system
|
||
setting_id = OGFSB00
|
||
instantiation = true
|
||
fan_max_speed = 60
|
||
filament_long_retractions_when_cut = 1
|
||
filament_max_volumetric_speed = 16
|
||
filament_retraction_distances_when_cut = 18
|
||
slow_down_layer_time = 12
|
||
compatible_printers =
|
||
|
||
[filament:Bambu ABS-GF @System]
|
||
inherits = Bambu ABS-GF @base
|
||
from = system
|
||
setting_id = OGFSB50_00
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu Support for ABS @System]
|
||
inherits = Bambu Support for ABS @base
|
||
from = system
|
||
setting_id = OGFSS06_00
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:COEX ABS @System]
|
||
inherits = COEX ABS @base
|
||
from = system
|
||
setting_id = COXABS01
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 16
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:COEX ABS PRIME @System]
|
||
inherits = COEX ABS PRIME @base
|
||
from = system
|
||
setting_id = CXABSP09
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 16
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:FDplast ABS @System]
|
||
inherits = FDplast ABS @base
|
||
from = system
|
||
setting_id = ABS01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:NIT ABS @System]
|
||
inherits = NIT ABS @base
|
||
from = system
|
||
setting_id = ABS01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Overture ABS Basic @System]
|
||
inherits = Overture ABS Basic @base
|
||
from = system
|
||
setting_id = OVABS08
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 16
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:PolyLite ABS @System]
|
||
inherits = PolyLite ABS @base
|
||
from = system
|
||
setting_id = OGFSB60_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu ASA @System]
|
||
inherits = Bambu ASA @base
|
||
from = system
|
||
setting_id = OGFSB01_00
|
||
instantiation = true
|
||
fan_min_speed = 25
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu ASA-Aero @System]
|
||
inherits = Bambu ASA-Aero @base
|
||
from = system
|
||
setting_id = OGFSB02_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu ASA-CF @System]
|
||
inherits = Bambu ASA-CF @base
|
||
from = system
|
||
setting_id = OGFSB51_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:COEX ASA PRIME @System]
|
||
inherits = COEX ASA PRIME @base
|
||
from = system
|
||
setting_id = CXASAP04
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 16
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:Elas ASA @System]
|
||
inherits = Elas ASA @base
|
||
from = system
|
||
setting_id = OGFSB01_00
|
||
instantiation = true
|
||
fan_min_speed = 25
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Elegoo ASA @System]
|
||
inherits = Elegoo ASA @base
|
||
from = system
|
||
setting_id = OGFSE06_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Overture ASA @System]
|
||
inherits = Overture ASA @base
|
||
from = system
|
||
setting_id = OGFOT009
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 8
|
||
|
||
[filament:PolyLite ASA @System]
|
||
inherits = PolyLite ASA @base
|
||
from = system
|
||
setting_id = OGFSB61_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:FDplast HIPS @System]
|
||
inherits = FDplast HIPS @base
|
||
from = system
|
||
setting_id = HIPS01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:AliZ PA-CF @System]
|
||
inherits = AliZ PA-CF @base
|
||
from = system
|
||
setting_id = AliZGFSA04
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PA-CF @System]
|
||
inherits = Bambu PA-CF @base
|
||
from = system
|
||
setting_id = OGFSN00
|
||
instantiation = true
|
||
nozzle_temperature_initial_layer = 290
|
||
nozzle_temperature = 290
|
||
fan_max_speed = 30
|
||
fan_min_speed = 10
|
||
fan_cooling_layer_time = 5
|
||
full_fan_speed_layer = 2
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PA6-CF @System]
|
||
inherits = Bambu PA6-CF @base
|
||
from = system
|
||
setting_id = OGFSN05_02
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PA6-GF @System]
|
||
inherits = Bambu PA6-GF @base
|
||
from = system
|
||
setting_id = OGFSN08_00
|
||
instantiation = true
|
||
chamber_temperatures = 60
|
||
filament_max_volumetric_speed = 10.5
|
||
nozzle_temperature = 265
|
||
nozzle_temperature_initial_layer = 265
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PAHT-CF @System]
|
||
inherits = Bambu PAHT-CF @base
|
||
from = system
|
||
setting_id = OGFSN04
|
||
instantiation = true
|
||
chamber_temperatures = 60
|
||
compatible_printers =
|
||
|
||
[filament:Bambu Support For PA/PET @System]
|
||
inherits = Bambu Support For PA/PET @base
|
||
from = system
|
||
setting_id = OGFSS03_00
|
||
instantiation = true
|
||
chamber_temperatures = 60
|
||
compatible_printers =
|
||
|
||
[filament:Bambu Support G @System]
|
||
inherits = Bambu Support G @base
|
||
from = system
|
||
setting_id = OGFSS01
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:COEX NYLEX PA6-CF @System]
|
||
inherits = COEX NYLEX PA6-CF @base
|
||
from = system
|
||
setting_id = CXPACF23
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 11
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:Fiberon PA12-CF @System]
|
||
inherits = Fiberon PA12-CF @base
|
||
from = system
|
||
setting_id = OGFSL52_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Fiberon PA6-CF @System]
|
||
inherits = Fiberon PA6-CF @base
|
||
from = system
|
||
setting_id = OGFSL50_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Fiberon PA6-GF @System]
|
||
inherits = Fiberon PA6-GF @base
|
||
from = system
|
||
setting_id = OGFSL51_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Fiberon PA612-CF @System]
|
||
inherits = Fiberon PA612-CF @base
|
||
from = system
|
||
setting_id = OGFSL53_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PC @System]
|
||
inherits = Bambu PC @base
|
||
from = system
|
||
setting_id = OGFSC00
|
||
instantiation = true
|
||
fan_max_speed = 40
|
||
slow_down_layer_time = 12
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PC FR @System]
|
||
inherits = Bambu PC FR @base
|
||
from = system
|
||
setting_id = OGFSC01_00
|
||
instantiation = true
|
||
fan_max_speed = 40
|
||
slow_down_layer_time = 12
|
||
compatible_printers =
|
||
|
||
[filament:COEX PCTG PRIME @System]
|
||
inherits = COEX PCTG PRIME @base
|
||
from = system
|
||
setting_id = CXPCTG15
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 12
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:AliZ PETG @System]
|
||
inherits = AliZ PETG @base
|
||
from = system
|
||
setting_id = AliZGFSA04
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:AliZ PETG-CF @base]
|
||
inherits = AliZ PETG @base
|
||
from = system
|
||
filament_id = AZ01-1
|
||
instantiation = false
|
||
fan_cooling_layer_time = 30
|
||
overhang_fan_speed = 100
|
||
close_fan_the_first_x_layers = 2
|
||
enable_pressure_advance = 0
|
||
pressure_advance = 0.033
|
||
fan_max_speed = 35
|
||
fan_min_speed = 10
|
||
filament_cost = 49.9
|
||
filament_flow_ratio = 1
|
||
filament_max_volumetric_speed = 10
|
||
filament_type = PETG-CF
|
||
filament_vendor = Aliz
|
||
hot_plate_temp = 79
|
||
hot_plate_temp_initial_layer = 79
|
||
nozzle_temperature = 275
|
||
nozzle_temperature_initial_layer = 275
|
||
nozzle_temperature_range_high = 290
|
||
nozzle_temperature_range_low = 260
|
||
overhang_fan_threshold = 25%
|
||
slow_down_min_speed = 10
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:AliZ PETG-Metal @base]
|
||
inherits = AliZ PETG @base
|
||
from = system
|
||
filament_id = AZ01-2
|
||
instantiation = false
|
||
fan_cooling_layer_time = 30
|
||
overhang_fan_speed = 100
|
||
close_fan_the_first_x_layers = 2
|
||
enable_pressure_advance = 0
|
||
fan_max_speed = 80
|
||
fan_min_speed = 30
|
||
filament_cost = 49.9
|
||
filament_flow_ratio = 1
|
||
filament_max_volumetric_speed = 13
|
||
filament_vendor = Aliz
|
||
hot_plate_temp = 79
|
||
hot_plate_temp_initial_layer = 79
|
||
nozzle_temperature = 260
|
||
nozzle_temperature_initial_layer = 260
|
||
overhang_fan_threshold = 25%
|
||
pressure_advance = 0.036
|
||
slow_down_min_speed = 10
|
||
textured_plate_temp = 70
|
||
textured_plate_temp_initial_layer = 70
|
||
|
||
[filament:Bambu PET-CF @System]
|
||
inherits = Bambu PET-CF @base
|
||
from = system
|
||
setting_id = OGFST01
|
||
instantiation = true
|
||
reduce_fan_stop_start_freq = 0
|
||
slow_down_min_speed = 10
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PETG Basic @System]
|
||
inherits = Bambu PETG Basic @base
|
||
from = system
|
||
setting_id = OGFSG00_01
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 13
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PETG HF @System]
|
||
inherits = Bambu PETG HF @base
|
||
from = system
|
||
setting_id = OGFSG02_00
|
||
instantiation = true
|
||
fan_cooling_layer_time = 20
|
||
fan_min_speed = 20
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
overhang_fan_speed = 100
|
||
slow_down_layer_time = 10
|
||
slow_down_min_speed = 10
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PETG Translucent @System]
|
||
inherits = Bambu PETG Translucent @base
|
||
from = system
|
||
setting_id = OGFSG01_00
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_retraction_length = 0.3
|
||
slow_down_layer_time = 8
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PETG-CF @System]
|
||
inherits = Bambu PETG-CF @base
|
||
from = system
|
||
setting_id = OGFSG50_01
|
||
instantiation = true
|
||
fan_cooling_layer_time = 30
|
||
fan_max_speed = 40
|
||
fan_min_speed = 5
|
||
filament_long_retractions_when_cut = 1
|
||
filament_max_volumetric_speed = 11.5
|
||
filament_retraction_distances_when_cut = 18
|
||
overhang_fan_speed = 100
|
||
compatible_printers =
|
||
|
||
[filament:COEX PETG @System]
|
||
inherits = COEX PETG @base
|
||
from = system
|
||
setting_id = CXPETG13
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 16
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:Elas PETG Basic @System]
|
||
inherits = Elas PETG Basic @base
|
||
from = system
|
||
setting_id = OGFSG00_01
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 13
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Elegoo PETG PRO @System]
|
||
renamed_from = Elegoo PETG Pro @System
|
||
inherits = Elegoo PETG PRO @base
|
||
from = system
|
||
setting_id = OGFSE02_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Elegoo PETG-CF @System]
|
||
inherits = Elegoo PETG-CF @base
|
||
from = system
|
||
setting_id = OGFSE03_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Elegoo Rapid PETG @System]
|
||
inherits = Elegoo Rapid PETG @base
|
||
from = system
|
||
setting_id = OGFSE01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:FDplast PETG @System]
|
||
inherits = FDplast PETG @base
|
||
from = system
|
||
setting_id = PET01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Fiberon PET-CF @System]
|
||
inherits = Fiberon PET-CF @base
|
||
from = system
|
||
setting_id = OGFSL54_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Fiberon PETG-ESD @System]
|
||
inherits = Fiberon PETG-ESD @base
|
||
from = system
|
||
setting_id = OGFSL06_00
|
||
instantiation = true
|
||
filament_cost = 29.99
|
||
compatible_printers =
|
||
|
||
[filament:Fiberon PETG-rCF @System]
|
||
inherits = Fiberon PETG-rCF @base
|
||
from = system
|
||
setting_id = OGFSL55_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:NIT PETG @System]
|
||
inherits = NIT PETG @base
|
||
from = system
|
||
setting_id = PET01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:PolyLite PETG @System]
|
||
inherits = PolyLite PETG @base
|
||
from = system
|
||
setting_id = OGFSG60_00
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 11.5
|
||
nozzle_temperature_range_high = 270
|
||
compatible_printers =
|
||
|
||
[filament:SUNLU PETG @System]
|
||
inherits = SUNLU PETG @base
|
||
from = system
|
||
setting_id = OSNLS08
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 14
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:eSUN PETG @System]
|
||
inherits = eSUN PETG @base
|
||
from = system
|
||
setting_id = PET01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:AliZ PLA @System]
|
||
inherits = AliZ PLA @base
|
||
from = system
|
||
setting_id = AliZGFSA04
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Aero @System]
|
||
inherits = Bambu PLA Aero @base
|
||
from = system
|
||
setting_id = OGFSA11_01
|
||
instantiation = true
|
||
additional_cooling_fan_speed = 0
|
||
slow_down_layer_time = 8
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Basic @System]
|
||
inherits = Bambu PLA Basic @base
|
||
from = system
|
||
setting_id = OGFSA00
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 21
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Dynamic @System]
|
||
inherits = Bambu PLA Dynamic @base
|
||
from = system
|
||
setting_id = OGFSA13_00
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 21
|
||
filament_vendor = Bambu Lab
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Galaxy @System]
|
||
inherits = Bambu PLA Galaxy @base
|
||
from = system
|
||
setting_id = OGFSA15_00
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Glow @System]
|
||
inherits = Bambu PLA Glow @base
|
||
from = system
|
||
setting_id = OGFSA12_00
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Impact @System]
|
||
inherits = Bambu PLA Impact @base
|
||
from = system
|
||
setting_id = OGFSA03
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 23.2
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Marble @System]
|
||
inherits = Bambu PLA Marble @base
|
||
from = system
|
||
setting_id = OGFSA07_00
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Matte @System]
|
||
inherits = Bambu PLA Matte @base
|
||
from = system
|
||
setting_id = OGFSA01
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_max_volumetric_speed = 22
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Metal @System]
|
||
inherits = Bambu PLA Metal @base
|
||
from = system
|
||
setting_id = OGFSA02
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 21
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Silk @System]
|
||
inherits = Bambu PLA Silk @base
|
||
from = system
|
||
setting_id = OGFSA05_01
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Silk+ @System]
|
||
inherits = Bambu PLA Silk+ @base
|
||
from = system
|
||
setting_id = OGFSA06_00
|
||
instantiation = true
|
||
supertack_plate_temp = 35
|
||
supertack_plate_temp_initial_layer = 35
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Sparkle @System]
|
||
inherits = Bambu PLA Sparkle @base
|
||
from = system
|
||
setting_id = OGFSA08_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Tough @System]
|
||
inherits = Bambu PLA Tough @base
|
||
from = system
|
||
setting_id = OGFSA09_02
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 21
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA Wood @System]
|
||
inherits = Bambu PLA Wood @base
|
||
from = system
|
||
setting_id = OGFSA16_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PLA-CF @System]
|
||
inherits = Bambu PLA-CF @base
|
||
from = system
|
||
setting_id = OGFSA50_01
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_max_volumetric_speed = 15
|
||
filament_retraction_distances_when_cut = 18
|
||
nozzle_temperature = 230
|
||
nozzle_temperature_initial_layer = 230
|
||
compatible_printers =
|
||
|
||
[filament:Bambu Support For PLA @System]
|
||
inherits = Bambu Support For PLA @base
|
||
from = system
|
||
setting_id = OGFSS02_02
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu Support For PLA/PETG @System]
|
||
inherits = Bambu Support For PLA/PETG @base
|
||
from = system
|
||
setting_id = OGFSS05_00
|
||
instantiation = true
|
||
eng_plate_temp = 60
|
||
eng_plate_temp_initial_layer = 60
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Bambu Support W @System]
|
||
inherits = Bambu Support W @base
|
||
from = system
|
||
setting_id = OGFSS00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:COEX PLA @System]
|
||
inherits = COEX PLA @base
|
||
from = system
|
||
setting_id = C0XPLA02
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 18
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:COEX PLA PRIME @System]
|
||
inherits = COEX PLA PRIME @base
|
||
from = system
|
||
setting_id = C0XPLA08
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 15
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:Elas PLA Basic @System]
|
||
inherits = Elas PLA Basic @base
|
||
from = system
|
||
setting_id = OGFSA00
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 13
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Elas PLA Pro @System]
|
||
inherits = Elas PLA Pro @base
|
||
from = system
|
||
setting_id = OGFSA00
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 13
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:Elegoo PLA @System]
|
||
inherits = Elegoo PLA @base
|
||
from = system
|
||
setting_id = OGFSE04_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Elegoo Rapid PLA+ @System]
|
||
inherits = Elegoo Rapid PLA+ @base
|
||
from = system
|
||
setting_id = OGFSE05_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:FDplast PLA @System]
|
||
inherits = FDplast PLA @base
|
||
from = system
|
||
setting_id = PLA01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:FILL3D PLA Turbo @System]
|
||
setting_id = FILL3D001SYS
|
||
from = system
|
||
instantiation = true
|
||
inherits = FILL3D PLA Turbo @base
|
||
compatible_printers =
|
||
|
||
[filament:NIT PLA @System]
|
||
inherits = NIT PLA @base
|
||
from = system
|
||
setting_id = PLA01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Numakers PLA+ @System]
|
||
inherits = Numakers PLA+ @base
|
||
from = system
|
||
setting_id = ONMK00
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
filament_max_volumetric_speed = 18
|
||
compatible_printers =
|
||
|
||
[filament:Overture Air PLA @System]
|
||
inherits = Overture Air PLA @base
|
||
from = system
|
||
setting_id = OGFOT006
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Overture Easy PLA @System]
|
||
inherits = Overture Easy PLA @base
|
||
from = system
|
||
setting_id = OGFOT003
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Overture Matte PLA @System]
|
||
inherits = Overture Matte PLA @base
|
||
from = system
|
||
setting_id = OGFSL05_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Overture PLA @System]
|
||
inherits = Overture PLA @base
|
||
from = system
|
||
setting_id = OGFSL04_05
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Overture PLA Pro @System]
|
||
inherits = Overture PLA Pro @base
|
||
from = system
|
||
setting_id = OGFOT001
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Overture Rock PLA @System]
|
||
inherits = Overture Rock PLA @base
|
||
from = system
|
||
setting_id = OGFOT004
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Overture Silk PLA @System]
|
||
inherits = Overture Silk PLA @base
|
||
from = system
|
||
setting_id = OGFOT002
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Overture Super PLA+ @System]
|
||
inherits = Overture Super PLA+ @base
|
||
from = system
|
||
setting_id = OGFOT005
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma CoPE @System]
|
||
inherits = Panchroma CoPE @base
|
||
from = system
|
||
setting_id = OGFSPM016
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA @System]
|
||
inherits = Panchroma PLA @base
|
||
from = system
|
||
setting_id = OGFSPM001
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Celestial @System]
|
||
inherits = Panchroma PLA Celestial @base
|
||
from = system
|
||
setting_id = OGFSPM008
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Galaxy @System]
|
||
inherits = Panchroma PLA Galaxy @base
|
||
from = system
|
||
setting_id = OGFSPM007
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Glow @System]
|
||
inherits = Panchroma PLA Glow @base
|
||
from = system
|
||
setting_id = OGFSPM010
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Luminous @System]
|
||
inherits = Panchroma PLA Luminous @base
|
||
from = system
|
||
setting_id = OGFSPM011
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Marble @System]
|
||
inherits = Panchroma PLA Marble @base
|
||
from = system
|
||
setting_id = OGFSPM003
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Matte @System]
|
||
inherits = Panchroma PLA Matte @base
|
||
from = system
|
||
setting_id = GFSPM002
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Metallic @System]
|
||
inherits = Panchroma PLA Metallic @base
|
||
from = system
|
||
setting_id = OGFSPM012
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Neon @System]
|
||
inherits = Panchroma PLA Neon @base
|
||
from = system
|
||
setting_id = OGFSPM013
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Satin @System]
|
||
renamed_from = Panchroma PLA Stain @System
|
||
inherits = Panchroma PLA Satin @base
|
||
from = system
|
||
setting_id = OGFSPM005
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Silk @System]
|
||
inherits = Panchroma PLA Silk @base
|
||
from = system
|
||
setting_id = OGFSPM004
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
|
||
[filament:Panchroma PLA Starlight @System]
|
||
inherits = Panchroma PLA Starlight @base
|
||
from = system
|
||
setting_id = OGFSPM009
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Temp Shift @System]
|
||
inherits = Panchroma PLA Temp Shift @base
|
||
from = system
|
||
setting_id = OGFSPM015
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA Translucent @System]
|
||
inherits = Panchroma PLA Translucent @base
|
||
from = system
|
||
setting_id = OGFSPM006
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Panchroma PLA UV Shift @System]
|
||
inherits = Panchroma PLA UV Shift @base
|
||
from = system
|
||
setting_id = OGFSPM014
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:PolyLite Dual PLA @System]
|
||
renamed_from = PolyLite Dual PLA
|
||
inherits = PolyLite PLA @base
|
||
from = system
|
||
setting_id = O64868365
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:PolyLite PLA @System]
|
||
inherits = PolyLite PLA @base
|
||
from = system
|
||
setting_id = OGFSL19
|
||
filament_id = OGFL00
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 15
|
||
compatible_printers =
|
||
|
||
[filament:PolyLite PLA Pro @System]
|
||
inherits = PolyLite PLA Pro @base
|
||
from = system
|
||
setting_id = OGFSPM019
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:PolyTerra Dual PLA @System]
|
||
renamed_from = PolyTerra Dual PLA
|
||
inherits = PolyTerra PLA @base
|
||
from = system
|
||
setting_id = O1258005940
|
||
filament_id = OGFL00-1
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:PolyTerra PLA @System]
|
||
renamed_from = PolyTerra PLA
|
||
inherits = PolyTerra PLA @base
|
||
from = system
|
||
setting_id = OGFSL18
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 22
|
||
compatible_printers =
|
||
|
||
[filament:Polymaker HT-PLA @System]
|
||
inherits = Polymaker HT-PLA @base
|
||
from = system
|
||
setting_id = OGFSPM017
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:Polymaker HT-PLA-GF @System]
|
||
inherits = Polymaker HT-PLA-GF @base
|
||
from = system
|
||
setting_id = OGFSPM018
|
||
instantiation = true
|
||
filament_flow_ratio = 0.98
|
||
filament_max_volumetric_speed = 16
|
||
|
||
[filament:SUNLU PLA Marble @System]
|
||
inherits = SUNLU PLA Marble @base
|
||
from = system
|
||
setting_id = OSNLS06
|
||
instantiation = true
|
||
filament_long_retractions_when_cut = 1
|
||
filament_retraction_distances_when_cut = 18
|
||
compatible_printers =
|
||
|
||
[filament:SUNLU PLA Matte @System]
|
||
inherits = SUNLU PLA Matte @base
|
||
from = system
|
||
setting_id = OSNLS02
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:SUNLU PLA+ 2.0 @System]
|
||
inherits = SUNLU PLA+ 2.0 @base
|
||
from = system
|
||
setting_id = OSNLS04
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:SUNLU PLA+ @System]
|
||
inherits = SUNLU PLA+ @base
|
||
from = system
|
||
setting_id = OSNLS03
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:SUNLU Silk PLA+ @System]
|
||
inherits = SUNLU Silk PLA+ @base
|
||
from = system
|
||
setting_id = OSNLS05
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:SUNLU Wood PLA @System]
|
||
inherits = SUNLU Wood PLA @base
|
||
from = system
|
||
setting_id = OSNLS07
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Valment PLA @System]
|
||
inherits = Valment PLA @base
|
||
from = system
|
||
setting_id = VLMNT_01
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Valment PLA Galaxy @System]
|
||
inherits = Valment PLA Galaxy @base
|
||
from = system
|
||
setting_id = VLMNT_04
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Valment PLA Silk @System]
|
||
inherits = Valment PLA Silk @base
|
||
from = system
|
||
setting_id = VLMNT_02
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Valment PLA-CF @System]
|
||
inherits = Valment PLA-CF @base
|
||
from = system
|
||
setting_id = VLMNT_03
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:eSUN PLA+ @System]
|
||
inherits = eSUN PLA+ @base
|
||
from = system
|
||
setting_id = OGFSL03_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:eSUN PLA-Basic @System]
|
||
inherits = eSUN PLA-Basic @base
|
||
from = system
|
||
setting_id = OGFSL04_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:eSUN PLA-Marble @System]
|
||
inherits = eSUN PLA-Marble @base
|
||
from = system
|
||
setting_id = OGFSL06_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:eSUN PLA-Matte @System]
|
||
inherits = eSUN PLA-Matte @base
|
||
from = system
|
||
setting_id = OGFSL05_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:COEX PLA+Silk @base]
|
||
inherits = fdm_filament_pla_silk
|
||
from = system
|
||
filament_id = CXPLSB03
|
||
instantiation = false
|
||
filament_vendor = COEX 3D
|
||
filament_cost = 30.00
|
||
filament_density = 1.24
|
||
filament_type = PLA
|
||
filament_notes = Silk finish for aesthetic prints - slightly higher temperature than regular PLA
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 245
|
||
bed_temperature = 60
|
||
bed_temperature_initial_layer = 60
|
||
temperature_vitrification = 55
|
||
filament_max_volumetric_speed = 15
|
||
filament_retraction_minimum_travel = 2
|
||
filament_retract_before_wipe = 70%
|
||
filament_retract_layer_change = 1
|
||
filament_retract_when_changing_layer = 1
|
||
filament_retraction_length = 1.5
|
||
filament_retraction_speed = 45
|
||
filament_deretraction_speed = 40
|
||
filament_wipe = 1
|
||
filament_wipe_distance = 2
|
||
fan_min_speed = 100
|
||
fan_max_speed = 100
|
||
disable_fan_first_layers = 1
|
||
full_fan_speed_layer = 3
|
||
slow_down_layer_time = 5
|
||
slow_down_min_speed = 10
|
||
external_perimeter_speed = 50%
|
||
compatible_printers =
|
||
compatible_printers_condition =
|
||
compatible_prints =
|
||
compatible_prints_condition =
|
||
|
||
[filament:Generic PLA Silk @System]
|
||
renamed_from = Generic Silk PLA @System
|
||
inherits = fdm_filament_pla_silk
|
||
from = system
|
||
setting_id = OGFSL99_01
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 7.5
|
||
filament_retraction_length = 0.5
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PPA-CF @System]
|
||
inherits = Bambu PPA-CF @base
|
||
from = system
|
||
setting_id = OGFSN06_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu PVA @System]
|
||
inherits = Bambu PVA @base
|
||
from = system
|
||
setting_id = OGFSS04_00
|
||
instantiation = true
|
||
nozzle_temperature = 240
|
||
nozzle_temperature_initial_layer = 240
|
||
compatible_printers =
|
||
|
||
[filament:FDplast SBS @System]
|
||
inherits = FDplast SBS @base
|
||
from = system
|
||
setting_id = SBS01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Bambu TPU 95A @System]
|
||
inherits = Bambu TPU 95A @base
|
||
from = system
|
||
setting_id = OGFSU00
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 3.6
|
||
compatible_printers =
|
||
|
||
[filament:Bambu TPU 95A HF @System]
|
||
inherits = Bambu TPU 95A HF @base
|
||
from = system
|
||
setting_id = OGFSU00_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:COEX TPE 30D @System]
|
||
inherits = COEX TPE 30D @base
|
||
from = system
|
||
setting_id = C0X30D20
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 3.5
|
||
compatible_printers =
|
||
|
||
[filament:COEX TPE 40D @System]
|
||
inherits = COEX TPE 40D @base
|
||
from = system
|
||
setting_id = C0X40D18
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 5.5
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:COEX TPE 60D @System]
|
||
inherits = COEX TPE 60D @base
|
||
from = system
|
||
setting_id = C0X60D19
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 6.5
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:COEX TPU 60A @System]
|
||
inherits = COEX TPU 60A @base
|
||
from = system
|
||
setting_id = C0X60A17
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 1
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|
||
|
||
[filament:Elegoo TPU 95A @System]
|
||
inherits = Elegoo TPU 95A @base
|
||
from = system
|
||
setting_id = OGFSE07_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:FDplast TPU @System]
|
||
inherits = FDplast TPU @base
|
||
from = system
|
||
setting_id = TPU01_00
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:Overture TPU @System]
|
||
inherits = Overture TPU @base
|
||
from = system
|
||
setting_id = OGFOT008
|
||
instantiation = true
|
||
filament_flow_ratio = 0.95
|
||
filament_max_volumetric_speed = 8
|
||
|
||
[filament:AliZ PETG-CF @System]
|
||
inherits = AliZ PETG-CF @base
|
||
from = system
|
||
setting_id = AliZGFSG50
|
||
instantiation = true
|
||
|
||
[filament:AliZ PETG-Metal @System]
|
||
inherits = AliZ PETG-Metal @base
|
||
from = system
|
||
setting_id = AliZGFSG50
|
||
instantiation = true
|
||
compatible_printers =
|
||
|
||
[filament:COEX PLA+Silk @System]
|
||
inherits = COEX PLA+Silk @base
|
||
from = system
|
||
setting_id = C0XPLS03
|
||
instantiation = true
|
||
filament_max_volumetric_speed = 15
|
||
filament_long_retractions_when_cut = nil
|
||
filament_retraction_distances_when_cut = nil
|
||
compatible_printers =
|